TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 18 Mar 2009 16:31:41 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Rick Bell <[log in to unmask]>
Subject:
From:
Rick Bell <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (658 lines)
Werner,

We placed the adhesive on four corners and some cleared depopulated areas inside the ball array prior to smt device placement, and cured it during the reflow process.  Essentially, we didn't use it as an underfill, but more as an SMA.  Of your two choices, I guess that would be "before soldering".

Our initial temp cycle failures with no underfill were typical stress-initiated fractures on corner pins.  After adding the adhesive in this fashion, the parts passed 1k cycles.  We didn't evaluate failure mechanisms past that.

rb

________________________________
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, March 18, 2009 4:19 PM
To: [log in to unmask]; Rick Bell
Subject: Re: [TN] Underfill Application

Hi Amol,
When you say: "we elected to just do a corner bond approach"--what exactly do you mean? after or before soldering?

If after soldering, that may have helped the corner SJs, but how did it help all the others?










Werner






-----Original Message-----
From: Rick Bell <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, 18 Mar 2009 4:50 pm
Subject: Re: [TN] Underfill Application

Amol,










I have some admittedly limited experience with underfilling CSP's for increased





reliability.  Some answers to your questions:










1.) Our material selection initially was governed by a host of parameters--





reworkability (see next point), minimum dispense gap, process temperatures, cte





matching, filler content, etc.  In my experience, trying to get a reworkable





version will greatly limit your choices.










2.) We used a Loctite material, I believe it was 3549.  Please be aware that the





term "reworkable" is relative.  We tried using it on polyimide flex substrates,





and found its reworkability was a matter of interpretation.  Your mileage may





vary...










3.) We used an Asymtek dispense jet platform with very good results as far as





material deposition.  Our only inspection capability was outsourced CSAM..










4.) Pitfalls-- Our biggest issues were some minor problems with adhesion to the





substrate/device, and incomplete encapsulation of a given solder joint due to





poor capillary fill on our device (this has highly detrimental effects in temp





cycle).  My only advice there is that if you're going to attempt a full





encapsulation, have CSAM inspection available to verify your coverage, or some





very tight process controls once you have a benchmarked process.










In the end, we elected to just do a corner bond approach, rather than trying to





fully encapsulate the BGA array, and we had reasonable success in reliability





improvement.








































-----Original Message-----





From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Kane, Amol (349)





Sent: Wednesday, March 18, 2009 2:48 PM





To: [log in to unmask]<mailto:[log in to unmask]>





Subject: [TN] Underfill Application










Dear Technetters,





We are about the develop a process for underfilling BGAs for a high reliability





application. the underfill will be a rework able underfill. I wanted to poll the





technet on:





1.      Guidance on material selection





2.      most common materials being used out there and the process equipment





being used to do so.





3.      Common pitfalls and things to lookout for





4.      inspection techniques used to inspect the finished product





5.      a good source for info on underfilling (books, papers etc.,)










Thanks in advance.










Regards,





Amol






























WARNING:  Export Control





This document may contain technical data within the definition of the





International Traffic in Arms Regulations (ITAR), and subject to the Export





Control Laws of the U.S. Government.  Transfer of such data by any means to a





foreign person, whether in the United States or abroad, without proper export





authorization or other approval from the U.S. Department of State is





prohibited.











CONFIDENTIALITY NOTICE:





This e-mail, and any attachments, is for the sole use of the intended





recipient(s) and may contain information that is confidential and





protected from disclosure under the law. Any unauthorized review, use,





disclosure, or distribution is prohibited. If you are not the intended





recipient, please contact the sender by reply e-mail, and delete/destroy





all copies of the original message and attachments.





Thank you.










---------------------------------------------------





Technet Mail List provided as a service by IPC using LISTSERV 15.0





To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in





the BODY (NOT the subject field): SIGNOFF Technet





To temporarily halt or (re-start) delivery of Technet send e-mail to





[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)





To receive ONE mailing per day of all the posts: send e-mail to





[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest





Search the archives of previous posts at: http://listserv.ipc.org/archives





Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for





additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or





847-615-7100 ext.2815





-----------------------------------------------------










---------------------------------------------------





Technet Mail List provided as a service by IPC using LISTSERV 15.0





To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in





the BODY (NOT the subject field): SIGNOFF Technet





To temporarily halt or (re-start) delivery of Technet send e-mail to





[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)





To receive ONE mailing per day of all the posts: send e-mail to





[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest





Search the archives of previous posts at: http://listserv.ipc.org/archives





Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for





additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or





847-615-7100 ext.2815





-----------------------------------------------------





---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2