TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 12 Mar 2009 20:34:30 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Chris Mahanna <[log in to unmask]>
Subject:
From:
Chris Mahanna <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (137 lines)
I'm electrical, but have to play mechanical in the lab sometimes, so from experience:
You have to load the sample slow enough to get the cable up onto the stress/strain curve, down to necking, then fracture.  If the long homogenous part doesn't strain (deform) it will ALWAYS break at the crimp.
We test copper plating bath T&E on foil samples.  Without a dogbone pattern (strengthening the crimp) it is almost impossible, unless you've got stretchy copper.
So, if the spec. allows, slow down the cross-head speed and see if that fixes the problem.  That's not to say the crimp doesn't need to be looked at.

Chris

Chris Mahanna
Robisan Laboratory Inc.





-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jean-François Bissonnette
Sent: Wednesday, March 11, 2009 12:07 PM
To: [log in to unmask]
Subject: Re: [TN] Cable Pull Test specifications

In a previous life I use to do a lot of pull tests and usually the wires would break before the crimping area.  So I agree that the problem may be over-crimping.

I also use to test the strength of the wires alone, without crimps.  It was a reliable way to know if the crimps were good.  If the crimped test were way below single wire (if the wires broke and not pulled off of course) I knew we had problems of over crimping.

Jean-François Bissonnette

t : 450-967-7100 ext : 242

[log in to unmask]

www.digico.cc

P N'imprimer que si nécessaire - Print only if you must

-----Message d'origine-----
De : Temkin, Gregg [mailto:[log in to unmask]]
Envoyé : 11 mars 2009 11:24
À : [log in to unmask]
Objet : Re: [TN] Cable Pull Test specifications

Actually too tight a crimp is often the cause of such failures.  The Circular Mil Area of many high count stranded wires is often greater than that of its solid or low strand count equivalent.  Suggest you have them verify they're not over-crimping, and, if their tool is adjustable, see if they can back it off a little.

Gregg

-----Original Message-----
From: Forrester, Michael (H USA) [mailto:[log in to unmask]]
Sent: Wednesday, March 11, 2009 7:00 AM
To: [log in to unmask]
Subject: [TN] Cable Pull Test specifications

I have a cable vendor that states the following:

"Currently have issue with inconsistency of tensile strength of the
crimp using wire ULTRA-FLEX PVC 1251/14 BLACK, due to the flexibility of
this wire item and the large amount of strands, at 1050 strands at
44AWG. After conducting several pull tests found that the breaking
points all ranged from 44lbs to 49 lbs with no consistency. I then
conducted a pull test on a typical 14 AWG, 19 strand wire and the result
was 89 lbs for comparison purposes. Due to not being able to duplicate
the acceptable pull test from previous shipments and considering the
properties of this high stranded and flexible wire we feel it will not
consistently meet the UL 486 standard 14 AWG pull test requirement of
50lbs"

     During testing, the cable breaks right at the crimp.  Should the
cable be able to take the 50 lbs even though there are many fine strands
making up the
14 AWG wire?  Is the cable not crimped properly and only the outer
strands are taking the load cusing a "failure".  The vendor is looking
for a deviation to reduce the
pull test requirement to 45 lbs.  Since the Mil-T-7928 spec is 70 lbs
and the UL 486 spec is 50lbs, I'm not sure if the make-up of the wire
(fine strands) really factors in or the vendor needs to crimp tighter on
the cable to add strength?  Any comments would be welcomed.  Thank you.

Michael Forrester
Sr. Product Engineer

Siemens Healthcare Diagnostics
101 Silvermine Rd.
Brookfield, CT  06804
PH: (203) 740-6452


The attachment named   could not be scanned for viruses because it is a password protected file.
----------------------------------------------------------------------------
This message and any included attachments are from Siemens Medical Solutions
and are intended only for the addressee(s).
The information contained herein may include trade secrets or privileged or
otherwise confidential information. Unauthorized review, forwarding, printing,
copying, distributing, or using such information is strictly prohibited and may
be unlawful. If you received this message in error, or have reason to believe
you are not authorized to receive it, please promptly delete this message and
notify the sender by e-mail with a copy to [log in to unmask]

Thank you

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2