We use Kyzen DF-10....1 gallon lasts 5-6 months in our inline.
We get it from Amtech...datasheet is on their page but didn't see it on Kyzen.com.
http://www.amtechsolder.com/kyzen.html
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Thursday, March 12, 2009 9:29 AM
To: [log in to unmask]
Subject: [TN] Water tank foaming inhibitor
Dear Technos,
Anyone familiar with a substance from Dow Chemical, or any other, that would inhibit foaming in the wash tank of the in-line aqueous wash machines? I would appreciate the product name and eventually part#!
Of course, any pros and cons (does it contaminate) would also be appreciated.
Thanks,
Ioan Tempea, ing.
Ingénieur Principal Fabrication / Sr. Manufacturing Engineer
30 ans déjà! - Already 30 years!
950 rue Bergar, Laval, Québec, H7L 5A1
t : 450-967-7100 ext : 244
Mtl : 514-990-5762
f : 450-967-7444
[log in to unmask]
www.digico.cc <http://www.digico.cc/>
P N'imprimer que si nécessaire - Print only if you must
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|