We are experiencing de-wetting upon application. We are using a PVA coater
and using the same ratio, 1 to 1. The problem is that it is interment within
the same lot making it difficult to pin down.
Samples of bare boards as well as boards that coated fine and ones that
coated poorly have been sent out to a lab for eval.
Ted
-----Original Message-----
From: Tom P. Hummel [mailto:[log in to unmask]]
Sent: Thursday, February 05, 2009 2:45 PM
To: TechNet E-Mail Forum; Ted Tontis
Subject: RE: [TN] Coating material
We currently use HumiSeal 1B73AP thinned 1 to 1 with 521 in our PVA
machine and have not had any issues. Are you experiencing problems?
What type of automated machine are you using?
Thomas P. Hummel
Carlton Industries Corp
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------