And it is critical that only a certified operator perform the process,
to ensure the board is clean, dry, and cool.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Thursday, February 19, 2009 8:55 AM
To: [log in to unmask]
Subject: Re: [TN] Ultrasonic cleaner for PCB
The boards go into the 105 Deg. C oven for 20 minutes. That removes all
surface moisture and entrapped moisture in vias, etc. Then they are
allowed to cool to room temp, and back into the printer.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leif Erik Laerum
Sent: Thursday, February 19, 2009 7:56 AM
To: [log in to unmask]
Subject: Re: [TN] Ultrasonic cleaner for PCB
Richard,
A related note. How do you dry your boards after cleaning in the
ultrasonic cleaner? Do these cleaners come with a drying capability? We
are looking for a more efficient way of cleaning misprints.
Leif Erik Laerum
Quality Assurance Manager
Texas Memory Systems
[log in to unmask]
Tel: (713) 266-3200 x468
www.texmemsys.com
Stadem, Richard D. wrote:
> The best ultrasonic cleaners are made by Crest. They are not made by
> Branson.
> Crest cleaners are designed with the specific frequencies that are
> safe for cleaning electronics, and work beautifully for stencils and
> PWBs as well. My experience with Crest cleaners is that they work
> forever, with no diminishing over time. I certainly cannot say that
for Branson.
> No, I don't work for Crest, nor do I have any interest in the company.
> I just have used Crest many times at different companies for the past
> 30 years, and all of the ones I have ever purchased are still working.
> They make a really good product, and they are very knowledgeable
people.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Ray Kong
> Sent: Wednesday, February 18, 2009 5:19 PM
> To: [log in to unmask]
> Subject: [TN] Ultrasonic cleaner for PCB
>
> Hi all,
>
> Can someone recommend a ultrasonic cleaner for mis-print PCBs? Our
> board size is less than 8"x10"
>
> Thanks all in advance.
>
> Regards,
>
> Ted Kong
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|