Hi,
We have a doubt about the following requirement of J-STD:
"Solder shall wet the entire inside of a cup type terminal."
Is the "entire inside" the inner part of the pin or the back side of the cup?
We have some connectors (micro-D) where the cup is soldered more than
75% but the wire is not soldered into the hidden part of the pin. This condition
has been detected by X-Ray.
In my opinion, this condition corresponds with an uncontrolled soldering
process (risk), but anyway, we want to be sure if it is also a defect.
Best regards,
Juan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|