Doesn't look like any black pad sample I have ever seen.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Woolley, Mark D.
(Mark)
Sent: Wednesday, February 11, 2009 3:56 PM
To: [log in to unmask]
Subject: Re: [TN] CRACKED ENIG PADS
Werner,
These would be very big grains in the nickel. Is this possible that
this is the infamous "Black Pad" issue in profile?
mark
mark
Mark Woolley |PTRL Laboratory | Avaya | 1300 West 120th Ave |
Westminster, CO 80234
Voice (Lab): (303) 538-2166
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner engelmaier
Sent: Wednesday, February 11, 2009 1:52 PM
To: [log in to unmask]
Subject: Re: [TN] CRACKED ENIG PADS
Well, these are cracks alright.
Werner
-----Original Message-----
From: Steve Gregory <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, 11 Feb 2009 3:46 pm
Subject: Re: [TN] CRACKED ENIG PADS
Hi again Lee!
Got it! Here it is:
http://stevezeva.homestead.com/files/THROUGH_HOLE_CRACKS-3.jpg
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman
Sent: Wednesday, February 11, 2009 1:42 PM
To: [log in to unmask]
Subject: Re: [TN] CRACKED ENIG PADS
Victor, George, Vladimir, and Company
Steve should be attaching the cross-section photograph. Since I did not
supervise the cross-sectioning activity, I will not vouch on the quality
of the cross-section.
I do see a layer (crack?) between the ENIG plating and the copper
surface, but the report that I received indicated that there was "no
evidence of a lack of bonding" - the lab reports words. That layer
(crack?) seems more pronounced than similar ENIG cross-sections I have
seen.
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Wednesday, February 11, 2009 2:23 PM
To: [log in to unmask]
Subject: Re: [TN] CRACKED ENIG PADS
Can you share the photos of the cross section?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M.
Sent: Wednesday, February 11, 2009 12:51 PM
To: [log in to unmask]
Subject: Re: [TN] CRACKED ENIG PADS
Lee,
When you say "Evidently" that you have done cro
Lee,
When you say "Evidently" that you have done cross sectioning and see
that the cracks are only in the Ni and Au and not in the Cu? Since you
said "There was no evidence of a lack of bonding between the copper and
the ENIG finish" that implies to me that you did cross section but since
I wasn't sure I thought I'd ask.
Regards,
George
George M. Wenger
Andrew Wireless Solutions
Senior Principal FMA/Reliability Engineer 40 Technology Drive, Warren,
NJ 07059
(908) 546-4531 (Office) (732) 309-8964 (cell) [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, February 11, 2009 1:42 PM
To: [log in to unmask]
Subject: Re: [TN] CRACKED ENIG PADS
Hi Lee!
Have your pictures posted. They are here:
http://stevezeva.homestead.com/files/THROUGH_HOLE_CRACKS-1.jpg
http://stevezeva.homestead.com/files/THROUGH_HOLE_CRACKS-2.jpg
I have to let those that know more about plating than I do answer this
one...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman
Sent: Wednesday, February 11, 2009 12:20 PM
To: [log in to unmask]
Subject: [TN] CRACKED ENIG PADS
I have asked Steve to put up a pair of pictures I received. They are of
cracks within the ENIG finish of a PWB. I know that the board failed,
based on IPC-6011 and IPC-6012.
My question is what would cause the cracking? Evidently, it is in the
Nickel layer and the copper layer was not compromised. There was no
evidence of a lack of bonding between the copper and the ENIG finish.
These boards are fresh from the supplier.
Just curious...
Thanks in advance.
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
------------------------
This message is for the designated recipient only and may contain
privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender immediately
and delete the original. Any unauthorized use of this email is
prohibited.
------------------------------------------------------------------------
------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|