TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 6 Feb 2009 09:29:33 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-15; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (62 lines)
Dave

I hadn't realised that Colin Thwaites had published such a paper. I
believe that his research of the subject may have been instigated by
myself, following publication of the paper I presented at Inter/Nepcon
'69, in Brighton, England, 'New Aspects on the Solderability of Printed
Circuits'. Unfortunately, I no longer have a copy of the Technical
Proceedings but, as I remember it (40 years is a long time ago!!!), I
evoked the problems caused by both pumice and ScotchBrite cleaning,
whereby the abrasive particles were embedded into the copper pore
structure and then the copper was swaged over them. The only way they
could be released was with a light persulfate etch and forceful rinse,
without which dewetting was inevitable after abrasive cleaning.

Having written this, I then re-read what I wrote in Section 7.2.4 (p.
76) of my book and found that it's similar in essence but more complete,
so my aged memory can't be that bad! Whatever, abrasives and
solderability make poor bedmates!

Hope this helps.

Brian

David D. Hillman wrote:
> Hi gang! Ok, I am in search of a technical reference and my usual, "always 
> works" sources have failed me. I am looking for the following technical 
> reference:
> 
> Thwaites, C. J. and Mackay, C. A. , " Some Effects of Abrasive Cleaning on 
> the Solderability of Printed Circuits", Metal Finishing Journal, Sept. 
> 1968, pp. 291-294, (also may be listed as ITRI Publication 386)
> 
> 
> Anyone have a copy or can direct me to where a copy can be obtained? And 
> yes, I have sent a request to the ITRI folks already (International Tin 
> Research Institute)
> 
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2