TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 20 Feb 2009 08:20:01 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (128 lines)
A good description of dewetting would be non uniform coverage of thick and
thin solder layers, with high contact angles to the thick bits - just as you
described.

Regards
 
 
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Thursday, February 19, 2009 5:29 PM
To: [log in to unmask]
Subject: Re: [TN] dewetting

Hi Lou - here is a simple way of keeping the two terms straight: 

Nonwetting:a nonwetting solderability issue is when the solder does not 
"wet" or make a metallurgical bond with the surface you are trying to 
solder

Dewetting: a dewetting solderability issue is when the solder does initial 
"wet" and makes a metallurgical bond with the surface you are trying to 
solder but then puddles/retracts on that surface similar to an oil on 
water reaction.

If you inspect a nonwetting surface under the appropriate magnification, 
you can see that no metallurgical bond was ever establish in contrast to a 
dewetting surface which will have evidence of a metallurgical bond being 
made. In many cases, the contrast requires a microscope/ good 
magnification to seen. 

The JSTD-002C, Figure 2B, page 40,  has photos of dewetting and 
nonwetting. Hope this helps.

Dave Hillman
Rockwell Collins
[log in to unmask]



Louis Hart <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
02/19/2009 10:23 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Louis Hart <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] dewetting






TechNetters, would someone fluent in soldering and terminology please 
advise or comment? In the IPC T-50H definition of dewetting, there is 
mention of a 'thin coating of solder' on the base metal. Pictures of 
dewetting in A-600 appear to show exposed base metal. A customer is 
complaining about dewetting on some PCBs that have all surfaces covered 
with solder, thin in some regions, thick in others. I can't see clearly 
the contact angle between the thick solder and thinner areas, but it may 
not be much different from 90 degrees. To me, it appears solderability 
should be OK, but I want to understand the dewetting phenomenon better 
before discussing with the customer.

By what physical mechanism does dewetting occur? How does this mechanism 
differ from nonwetting?

Thanks for any guidance...Louis

Louis Hart
Compunetics
Monroeville, PA
USA
[log in to unmask]<mailto:[log in to unmask]>
412-858-1272


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2