Good morning, we are receiving laser marked 2D barcode from 2 suppliers
in high volume, no issues. We tried inkjet. Hard to read consistently,
can contaminate solderable surfaces, high maintenance if used in high
volume.
Best regards, Wolfgang
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stewart, Dougal
Sent: Thursday, February 12, 2009 11:31 AM
To: [log in to unmask]
Subject: Re: [TN] 2-D Laser Etch Barcodes on PCBs
Sorry to disappoint you Brian, but laser marking pcbs in the fab process
is not a common feature anywhere. What is now possible is to ink jet
print a unique barcode to every board, and this is indeed becoming a
mature process with more and more fabricators able to provide as an
additional service.
regards
Dougal
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Chandler
Sent: 12 February 2009 15:53
To: [log in to unmask]
Subject: [TN] 2-D Laser Etch Barcodes on PCBs
How common is it to have the PCB supplier etch a unique 2-D barcode on
the PCB using a laser? We seem to have trouble finding PCB suppliers
with this capability. I would think this is a very mature process and
quite common.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
Stevenage Circuits Limited.
Registered office: Caxton Way, Stevenage, Hertfordshire, SG1 2DF.
Registered in England under company number 1059497.
The views of the author may not necessarily represent those of Stevenage
Circuits Ltd.
This message may contain information and/or data that is confidential
and legally privileged.
It is intended solely for the addressee(s) only.
If you are not the intended recipient you are notified that any use,
publication, reproduction or dissemination is strictly prohibited.
In such an event, please contact the sender by return e-mail and destroy
this and all copies of this message and/or data.
Please be aware that the integrity of this email cannot be guaranteed,
as it is not a safe and secure medium for communication.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|