Hi Bev and fellow Techies
Yes it is being changed both for IPC and IEC.
The recommended temperature for lead-free is presently under
consideration at 180DegC.
IPC-J-STD005 is under A Rev and the committee will be meeting to
review some RR testing we are completing in time for APEX in Las Vegas.
I hope this helps
Graham Naisbitt
Gen3 Systems
On 19 Feb 2009, at 20:41, Bev Christian wrote:
> Technetters,
> I would like your opinion on this.
>
> IPC-TM-650, Method 2.4.35 Solder Paste - Slump Test--1/95 states that
> hot slump is measured after exposure to 150C for 10 to 15 minutes. Do
> you think this should be changed for lead free solder pastes?
> Bev
> RIM
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain
> confidential information, privileged material (including material
> protected by the solicitor-client or other applicable privileges),
> or constitute non-public information. Any use of this information by
> anyone other than the intended recipient is prohibited. If you have
> received this transmission in error, please immediately reply to the
> sender and delete this information from your system. Use,
> dissemination, distribution, or reproduction of this transmission by
> unintended recipients is not authorized and may be unlawful.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]
> : SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]
> : SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask]
> or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|