Try adding more thinner to eliminate the webbing. The 1 to 1 on their
datasheet is just a starting point.
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ted Tontis
Sent: Friday, February 06, 2009 8:26 AM
To: [log in to unmask]
Subject: Re: [TN] Coating material
Grunde,
The HumiSeal 1B73AP is supposed to reduce the occurrence of webbing,
that's
why it was original chosen. Now that we switched over to the 1B73 we are
seeing signs of it and trying to stay on top of it. We reduced the
atomizer
a little to try to keep it to a minimum, I am not sure how much that is
going to help. I have seen worse on one of our other coaters spraying
HumiSeal 905. We are currently using a PVA coater and spraying it on.
Ted
_____
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Friday, February 06, 2009 2:01 AM
To: TechNet E-Mail Forum; Ted Tontis
Cc: [log in to unmask]
Subject: Re: [TN] Coating material
Hi
Small air bubbles and cobwebbing are familiar issues with these
materials.
Do you use spray or filmcoating?
Cheers, Grunde
Is anyone currently using HumiSeal 1B73AP mixed with 521 carrier in a
automated process? If so have you noticed any coating issues?
Thank you,
Ted Tontis CID
Quality Engineer
Borg Indak, Inc.
701 Enterprise Dr
Delavan, WI 53115
C 262-949-8887
P 262-245-3060
F 262-728-3788
[log in to unmask]
www.borgindak.com <http://www.borgindak.com/>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|