Here are a couple pages from my training wall charts on BGA inspection of
high temp balls and plastic ball joints. They show similar views as Steve's
image.
Optical and x-ray inspection www.ASKbobwillis.com/balls.pdf
I understand that IPC610E will feature both high temp balls and columns in
the future with criteria and more detailed criteria for standard BGA
packages.
Many thanks
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
New Bob Willis "Printed Board Inspection & Quality Control Workshop" 24th
March www.ASKbobwillis.com/faworkshops.pdf
"Troubleshooting Your Assembly Yields Workshop" 25th March
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 22nd April
www.ASKbobwillis.com/faworkshops.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: 27 February 2009 18:28
To: [log in to unmask]
Subject: Re: [TN] Reflowing CBGA component (with high Sn balls) using
Eutectic solder paste
Hi All!
Dave is right, the balls are Pb90Sn10 according to IBM's package
description in this document:
http://tinyurl.com/da4cot
We build a lot of boards that use this device, and the joints do look a
lot different than other BGA's that have eutectic balls. There will be a
very noticable demarcation line between the solderjoint and ball itself.
Here's what our joints look like:
http://stevezeva.homestead.com/files/PowerPC_Joints.jpg
The board isn't ENIG like Joe's, it's HASL. My peak temperatures range
from 218 C. to 226 C., and my TAL ranges from 75-seconds to 81-seconds
depending on which thermocouple you're looking at in my temperature
plot.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Friday, February 27, 2009 10:44 AM
To: [log in to unmask]
Subject: Re: [TN] Reflowing CBGA component (with high Sn balls) using
Eutectic solder paste
Hi Joe - could you please check your solder alloy element ratio, did you
really mean Pb90Sn10? The Sn90Pb10 begins melting at 183C and the
Pb90Sn10 begins melting at 268C. I am not familiar with CBGA using a
Sn90Pb10 ratio.
Dave Hillman
Rockwell Collins
[log in to unmask]
Joe Macko <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/27/2009 10:03 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] Reflowing CBGA component (with high Sn balls) using Eutectic solder
paste
Hi All,
My question is related to the soldering of IBM PPC CBGAs type components
(that have Sn90Pb10 solder balls) using Sn63 paste onto ENIG finished
boards. What are the "determining-factors" to improve the
wetting/diffusion of the eutectic solder paste into the high Sn solder
balls. The eutectic solder appears to wet well to the ENIG pads located
on the board but occasionally I see eutectic solder fillets that do not
always appear to fuse well with the high Sn content balls (if fuse is
the correct word?). thx
Best Regards,
-Joe
"This e-mail and any attachments are solely for the use of the addressee
and may contain L-3 proprietary information that may also be defined as
U.S. Government export controlled technical data. If you are an
unintended
recipient of this e-mail, use, disclosure or distribution of its content
is prohibited. Please notify the sender by return e-mail and immediately
delete this message."
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|