Dave,
We actually put in a piece of lead. The peak for lead is slightly offset from where we find the peak.
Doctors Turbini and Koo came by with a couple of suggestions:
Turbini - some Bi compounds used as catalysts for polymerization
Koo - Bi amine halides used as flame retardants
Great when I have staff like this! Should have gone to them first before TechNet, but at least we all learn this way. :)
Bev
RIM
________________________________
From: [log in to unmask]
To: TechNet E-Mail Forum ; Bev Christian
Cc: [log in to unmask]
Sent: Thu Feb 26 12:23:37 2009
Subject: Re: [TN] Weird one - bismuth in overmold
Hi Bev - hey, Bismuth and Lead shell lines overlap each other in the 0-10kV range but are distinctly separate in the 10-20kV range. Which range did you use? Could you have a case of mistaken identity?
Dave Hillman
Rockwell Collins
[log in to unmask]
Bev Christian <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/26/2009 09:51 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bev Christian <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Weird one - bismuth in overmold
TechNetters,
In checking a component for one thing or another we found via SEM/EDX
particles of bismuth in the overmold. Smaller amounts of bromine were
also found in the same spots but the largest signal by far was due to
Bi. I have never seen or heard of such a thing before. Can anyone shed
any light on this before I go to the component vendor?
Bev
RIM
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
|
|
|