Many thanks Keith I have one of those also in my library, see this link
below, but I would never have imagined this to be called a fish eye!!! The
example shows some bubbles but also some sunken areas in the coating. Link
is www.ASKbobwillis.com/fisheye.pdf
Reading through a NASA document it refers to the defect as:
Fisheye A small area of a fabric that resists resin wetting that can be
caused by resin system, fabric and treating.
Still confused from Chelmsford and not totally convinced everyone has the
same vision of a fisheye
Have a great Friday and weekend
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
New Bob Willis "Printed Board Inspection & Quality Control Workshop" 24th
March www.ASKbobwillis.com/faworkshops.pdf
"Troubleshooting Your Assembly Yields Workshop" 25th March
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 22nd April
www.ASKbobwillis.com/faworkshops.pdf
-----Original Message-----
From: Keith Calhoun [mailto:[log in to unmask]]
Sent: 20 February 2009 16:08
To: TechNet E-Mail Forum; Bob Willis
Subject: RE: [TN] Conformal Coating Inspection
Bob;
I don't have any pictures of conformal coating that exhibits "fisheyes"
but found this link to a finishing site that does explain it and show an
example in a painted finish.
http://www.specialchem4coatings.com/tc/surface_modification/?id=fish_eye
s
Keith S. Calhoun
Product Engineer
SoPark Corporation
3300 South Park Avenue
Buffalo, New York 14218
Phone: 716-822-0434 Ext. 237
Fax: 716-822-5062
email: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Willis
Sent: Friday, February 20, 2009 10:52 AM
To: [log in to unmask]
Subject: [TN] Conformal Coating Inspection
I have been putting together some inspection standards for a new
workshop in Germany. I have found a number of references to "Fish Eyes"
but never seen an example. It's a common term but seems to be elusive in
terms of actual examples.
Would the images at the following link be considered "Fish Eyes" by
users or are we looking for more subtle examples like two bubbles
between IC leads??
www.ASKbobwillis.com/gonefishing.pdf
Many thanks
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
New Bob Willis "Printed Board Inspection & Quality Control Workshop"
24th March www.ASKbobwillis.com/faworkshops.pdf
"Troubleshooting Your Assembly Yields Workshop" 25th March
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 22nd April
www.ASKbobwillis.com/faworkshops.pdf
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|