We use a UV curable solder mask for the PCB repairs our fir
Dear Ioan:
We use a UV curable solder mask for the PCB repairs our firm performs.
If it gets to more than a few areas (read 3-4) then the time it takes to do this manually underneath a microscope becomes too cost prohibitive. We then go to a stay-in-place stencil which "band aids" the mask. With this method you really have to make sure the stencil pattern is very tight to the vias/dogbone. The GERBER data of the site needs to be used to get this right.
We have seen mask underneath BGAs wich is so severely udercut or has such poor adhesion that no matter what you do you are fighting a losing battle.
Bob Wettermann
________________________________
From: Ioan Tempea <[log in to unmask]>
To: [log in to unmask]
Sent: Friday, February 20, 2009 7:47:01 AM
Subject: [TN] Repair soldermask
Hello Technos,
What kind of soldermask do you use for repair jobs under BGAs? You know, the original SM goes away when wicking the pads after BGA removal and we need to cover the vias back. And I'm talking lead-free.
Thank you,
Ioan Tempea, ing.
Ingénieur Principal Fabrication / Sr. Manufacturing Engineer
30 ans déjà! - Already 30 years!
950 rue Bergar, Laval, Québec, H7L 5A1
t : 450-967-7100 ext : 244
Mtl : 514-990-5762
f : 450-967-7444
[log in to unmask]
www.digico.cc <http://www.digico.cc/>
P N'imprimer que si nécessaire - Print only if you must
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|