TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 17 Feb 2009 13:50:58 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (68 lines)
NiCr, correct. You start deposition of a few nm NiCr layer on the PET film, then you add Al to a thickness of some um, then roll the cigar.  NiCr does not melt until some 2300F, depending on what W%.
Inge

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz
Sent: tisdag 17 februari 2009 01:01
To: [log in to unmask]
Subject: Re: [TN] Capacitor construction - foil alloy question

Carl, you might have your friend check for tantalum - a common electrode in some capacitors.? A more modern replacement for scarce tantalum is niobium.?A quick check says that both of these melt at over 4000 F.? ?Just a thought. 

Denny Fritz


-----Original Message-----
From: Carl VanWormer <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, 16 Feb 2009 9:46 am
Subject: [TN] Capacitor construction - foil alloy question



This came from a friend, but I couldn't answer, so I thought of the TechNet search engine.  Can "you guys" suggest a source of information to answer this question?

I've got a strange situation. The contents of a steel enclosure were recovered after a large fire. The copper and brass components were melted and fused. BUT the spiral foil from a capacitor survived inside the same steel box. I ASSUMED it was aluminum which creates a nasty conundrum: copper melts at 1860F, Aluminum at 1180F. BUT I've been informed (to my chagrin) that "newer high quality" 
capacitors use a nickel chromium alloy foil - do you have any experience with this?? A quick Google search didn't turn up any immediately recognizable information...

Thanks,
Carl



Carl Van Wormer, P.E.
Senior Hardware Engineer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR  97006
Cipher Systems (503) 617-7447   
Direct Line (503) 425-5163

This message may contain confidential and/or proprietary information, and is intended for the person/entity to whom it was originally addressed. Any use by others is strictly prohibited.



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2