TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Date:
Sun, 8 Feb 2009 11:09:30 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<008f01c9897e$de898990$6f02fea9@ingemar1446736>
Content-Type:
text/plain; charset=ISO-8859-15; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (335 lines)
Sorry to disappoint you, Inge. I've seen every single building in the 
Vatican!

OK, from a plane on its approach to Rome airport! :-D

Can't say I've ever met Joseph Alois Ratzinger, though, and I'm not even 
sure I'd want to as I'm not exactly on the same theological wavelength 
as his. I think the only thing we have in common is that we are both old 
men and we have both had age-related strokes and we would both be better 
keeping our mouths tightly shut. I don't think that is exactly the best 
basis for a good friendship. Can I call him Joe?

Oh! I've just remembered that someone in Germany used to call me the 
Reinigung Papst, so perhaps I'm on a par with Benedict the umpteenth??? :-D

Brian

Inge wrote:
> Brian is wise as a guru, and he seems to have a finger in affairs all over
> this century. To change a popular fun story, I exchange some names. Here it
> goes.
> 
> Let one of the persons be Bev and the other Brian. Walking on the street in
> the big town, Bev notices that many persons nod at Brian or shout from the
> other side 'Hi Brian', and Brian waves his hand. This is repeated even next
> and following day, Bev being a little annoyed: -Brian you seem to know
> everybody.  -Yes I do.
> 
> -Hmm.. but you don't know the taxi driver coming this way just now.
> Taxi driver : -Hello Brian!
> Beve: -just a coincident. However, we pass one of Lenovo's offices in a
> minute, you don't know any bosses there.
> When they  pass the entrance of that building, a gentleman appears and 
> heads
> for a big limosine, hesitates a second and waves at Brian: -Hello Brian!
> The  man was Simon Shum Siu-hung, CEO.
> Bev gets something wild in his eyes, neck being red: - That was in this
> town, on the other side of the sea you are quite unknown.
> Brian shrugs: -Know most there too.
> Bev:- you make me angry, you..you....braggart. Then let's go to Italy and
> see what kind of guy you are to them.
> So, some days later, they are in Roma. A caravan of state deputy cars
> appears suddenly, escorted by motorcycle police. The second car stops for a
> moment, door opens a little and small figure puts his head out and
> shouts: -Hi Brian, are you going to see the Pope? Sorry, can't stop here,
> see you later.
> It was Mr Berlusconi.
> Bev has not given in, hissing at Brian: -See the Pope, most stupid I've
> heard, you must be at least a states leader to get audience.
> Brian: - I know, so I use to call him only.
> Next day, it happens to be a day when the Pope is speaking to the people
> from his balcony, and Bev has dragged Brian with him: - Now, you little
> lier, prove that you know the holy man on the balcony.
> Brian: - Well, no problems. Wait here, I'll step up to His Highness and 
> as a
> sign, I will have my hand on his shoulder and wave at you.
> And so it came to be, but suddenly Brian can see that Bev, down there, 
> falls
> to the ground and does not rise. So, Brian says to the Pope: - John, I 
> have to leave, something happened to my friend Bev.
> John: -Pax vobiscum, Brian.
> At place, Brian gets Bev on feet and asks what the heck he was fancy for:
> Bev:- You see, Brian, a guy standing beside me asked me this ' Up there 
> on the balcony, all know Brian, but who is he standing beside?
> 
> Dont take this litterally, Brian is well known only in Switzerland, 
> Cyprus, England, Germany, Netherlands, the US and some more places, but 
> he is probably not that familiar with the Vatican.
> 
> Inge
> 
> 
> 
> ----- Original Message ----- From: "Brian Ellis" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Friday, February 06, 2009 3:29 PM
> Subject: Re: [TN] In Search of a Technical Reference
> 
> 
>> Hey, don't forget that in the civilised world, an eraser is called a
>> rubber. In fact that's how caoutchouc got its name, because it was first
>> used for rubbing out mistakes when writing. Nothing to do with friction
>> between men and women, even when they live in condominiums!
>>
>> Brian
>>
>> David D. Hillman wrote:
>>> Hi Mike, Brian and gang!  I'll go chase down Brian's InterNepcon '69
>>> paper and the book chapter segment. Our Rockwell Collin's Technical
>>> Reference database is pretty extensive but I was striking out on this
>>> one. I haven't heard back from ITRI yet and was getting impatient so I
>>> thought I would ask TechNet for help. The reason I am chasing that
>>> reference is that I have finally gotten feed up with addressing the 
>>> issue
>>> of well intended but misguided internal/external customers using "Pearl
>>> Pink" erasers as a surface finish oxide/discoloration removal protocol.
>>> The pink erasers come from multiple sources, have uncharacterized
>>> chemical compositions and leave contamination on the printed board
>>> surfaces that have been "cleaned". My co-op students and I have 
>>> completed
>>> a small investigation demonstrating the issues using SEM and FTIR 
>>> results
>>> on a variety of printed wiring board surface finishes and now I am just
>>> pulling together the external data sets on the topic that other
>>> investigators have published. Oddly, it seems to be a topic that 
>>> everyone
>>> fully understood in the late '60s but has been erased (what a pun!) from
>>> the industry tribal knowledge pool. The pumice and ScotchBrite
>>> information has been captured in the external data sets as well so I am
>>> going to include that information in the our paper. Probably something
>>> that I'll publish at one of the IPC or SMTA conferences.  Looks like 
>>> I'll
>>> be giving the TechNet an acknowledgement for everyone's most valuable
>>> assistance! Thanks to everyone for their assistance - TechNet is such a
>>> great tool!
>>>
>>> Dave
>>>
>>>
>>>
>>> Mike Fenner <[log in to unmask]> Sent by: TechNet <[log in to unmask]>
>>> 02/06/2009 06:04 AM
>>> Please respond to
>>> [log in to unmask]
>>>
>>>
>>> To
>>> [log in to unmask]
>>> cc
>>>
>>> Subject
>>> Re: [TN] In Search of a Technical Reference
>>>
>>>
>>>
>>>
>>>
>>>
>>> I remember Colin Thwaites's paper very well and Brian's, was grateful 
>>> for
>>> them, but no longer have copies. I would be surprised if the ITRI people
>>> don't find a copy. I asked them for
>>> an actual reference to some information of the industry legend type -
>>> meaning everyone knows it but not why or how they know it - and they
>>> found
>>> first references in early 1940s. Regards
>>>  Mike
>>> -----Original Message-----
>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
>>> Sent: Friday, February 06, 2009 7:30 AM
>>> To: [log in to unmask]
>>> Subject: Re: [TN] In Search of a Technical Reference
>>>
>>> Dave
>>>
>>> I hadn't realised that Colin Thwaites had published such a paper. I
>>> believe that his research of the subject may have been instigated by
>>> myself, following publication of the paper I presented at Inter/Nepcon
>>> '69, in Brighton, England, 'New Aspects on the Solderability of Printed
>>> Circuits'. Unfortunately, I no longer have a copy of the Technical
>>> Proceedings but, as I remember it (40 years is a long time ago!!!), I
>>> evoked the problems caused by both pumice and ScotchBrite cleaning,
>>> whereby the abrasive particles were embedded into the copper pore
>>> structure and then the copper was swaged over them. The only way they
>>> could be released was with a light persulfate etch and forceful rinse,
>>> without which dewetting was inevitable after abrasive cleaning.
>>>
>>> Having written this, I then re-read what I wrote in Section 7.2.4 (p.
>>> 76) of my book and found that it's similar in essence but more complete,
>>> so my aged memory can't be that bad! Whatever, abrasives and
>>> solderability make poor bedmates!
>>>
>>> Hope this helps.
>>>
>>> Brian
>>>
>>> David D. Hillman wrote:
>>>> Hi gang! Ok, I am in search of a technical reference and my usual,
>>> "always
>>>
>>>> works" sources have failed me. I am looking for the following technical
>>>> reference:
>>>>
>>>> Thwaites, C. J. and Mackay, C. A. , " Some Effects of Abrasive Cleaning
>>> on
>>>
>>>> the Solderability of Printed Circuits", Metal Finishing Journal, Sept.
>>>> 1968, pp. 291-294, (also may be listed as ITRI Publication 386)
>>>>
>>>>
>>>> Anyone have a copy or can direct me to where a copy can be obtained? 
>>>> And
>>>
>>>> yes, I have sent a request to the ITRI folks already (International Tin
>>>> Research Institute)
>>>>
>>>> Dave Hillman
>>>> Rockwell Collins
>>>> [log in to unmask]
>>>>
>>>> ---------------------------------------------------
>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>> To unsubscribe, send a message to [log in to unmask] with following text
>>> in
>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>> To receive ONE mailing per day of all the posts: send e-mail to
>>> [log in to unmask]: SET Technet Digest
>>>> Search the archives of previous posts at:
>>> http://listserv.ipc.org/archives
>>>> Please visit IPC web site
>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>> for additional information, or contact Keach Sasamori at [log in to unmask]
>>> or
>>> 847-615-7100 ext.2815
>>>> -----------------------------------------------------
>>>>
>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following 
>>> text in
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to
>>> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at:
>>> http://listserv.ipc.org/archives
>>> Please visit IPC web site
>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>> for additional information, or contact Keach Sasamori at [log in to unmask]
>>> or
>>> 847-615-7100 ext.2815
>>> -----------------------------------------------------
>>>
>>>
>>> ***This email, its content, and any files transmitted with it, are
>>> intended solely for the addressee(s) and may be legally privileged 
>>> and/or
>>> confidential. If you are not the intended recipient, please contact the
>>> sender by return and delete the material from any computer. Any review,
>>> retransmission, dissemination, or other use of, or taking of any action
>>> in reliance upon this information by persons or entities other than the
>>> intended recipient is prohibited.
>>>
>>> Messages sent via this medium may be subjected to delays, non-delivery,
>>> and unauthorized alteration. This email has been prepared using
>>> information believed by the author to be reliable and accurate, but
>>> Indium Corporation makes no warranty as to accuracy or completeness.
>>> Indium Corporation does not accept responsibility for changes made to
>>> this email after is was sent. Any opinions or recommendations expressed
>>> herein are solely those of the author. They may be subject to change
>>> without notice.***
>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following 
>>> text in
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to
>>> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at:
>>> http://listserv.ipc.org/archives
>>> Please visit IPC web site
>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>>> ext.2815
>>> -----------------------------------------------------
>>>
>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following 
>>> text in
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to
>>> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at:
>>> http://listserv.ipc.org/archives
>>> Please visit IPC web site
>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>>> ext.2815
>>> -----------------------------------------------------
>>>
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: 
>> http://listserv.ipc.org/archives
>> Please visit IPC web site 
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at 
>> [log in to unmask] or
>> 847-615-7100 ext.2815
>> ----------------------------------------------------- 
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
> ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2