Nice thing about Florida winters is we can back off from SPF50 to SPF35 sunblock
Bob
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner engelmaier
Sent: Thursday, January 15, 2009 11:13 AM
To: [log in to unmask]
Subject: Re: [TN] NTC RE: [TN] Possible cause on open
Wet suit is good anyway--avoids the sun burn.
Werner
-----Original Message-----
From: Graham Collins <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, 15 Jan 2009 10:43 am
Subject: Re: [TN] NTC RE: [TN] Possible cause on open
But Werner, you'd have to wear a wet suit, otherwise there would be serious shrinkage issues with just a speedo on! Oh, the horror!
regards,
- Graham
(-17 C here in Halifax)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner engelmaier
Sent: Thursday, January 15, 2009 11:33 AM
To: [log in to unmask]
Subject: Re: [TN] NTC RE: [TN] Possible cause on open
Not so--no problem starting the boat.
werner
-----Original Message-----
From: Ian Hanna <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, 15 Jan 2009 9:59 am
Subject: Re: [TN] NTC RE: [TN] Possible cause on open
The skiing sure must suck...
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Croslin, Robert
Sent: Thursday, January 15, 2009 9:50 AM
To: [log in to unmask]
Subject: Re: [TN] NTC RE: [TN] Possible cause on open
Whiners! It was all the way down to 39° last night here in Florida.
Bob Croslin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Thursday, January 15, 2009 9:12 AM
To: [log in to unmask]
Subject: [TN] NTC RE: [TN] Possible cause on open
Beatcha!
-20C with no wind at 6 AM.
It's not called the Gr
eat White North for nothing!
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, January 15, 2009 8:05 AM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open
Mornin' Everbody!
Well, here in Tulsa, we're just like a lot of other people in the country this
morning, trying to stay warm. Right now we're sitting at -10 C. with a wind
chill of -15 C. It's supposed to be colder tomorrow...
GA, I have your pictures posted now. They're at:
http://stevezeva.homestead.com/files/Fracture1.jpg
http://stevezeva.homestead.com/files/Fracture2.jpg
Hopefully someone can give you some ideas...
Steve=0
A
________________________________
From: Tan Geok Ang [mailto:[log in to unmask]]
Sent: Wednesday, January 14, 2009 7:27 PM
To: [log in to unmask]; Steve Gregory
Subject: Possible cause on open
Hi Steve,
Please help to download these pictures TechNet, thanks.
Hi All experts,
Testing (combine test of 16G at 85 oC) was performed on evaluation
boards with under-filled BGAs. Open issue (cracks) was detected only at some
corners of the BGA (35x35mm with 1156 balls) after the test. Lead-free process
and PCB with ENIG surface finish. Peak temperature is 248 oC with a 65 sec above
217 oC.
FYI, the service lab has not come out a report.
What are the possible causes? (CET mismatches, Lead-free alloy
related, material, pr
ocesses)
Thank you in advance.
Regards
GA Tan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the BODY
(NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start)
delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of
all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for a dditional information, or
contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error, please
immediately reply to the sender and delete this information from your system.
Use, dissemination, distribution, or reproduction of this transmission by
unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a=2
0service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the BODY
(NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start)
delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of
all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail Li
st provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a
message to [log in to unmask] with following text in the BODY (NOT the subject
field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet
send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of
all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to L
[log in to unmask] with following text in the BODY
(NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start)
delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of
all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the BODY
(NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start)
delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or
(MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject20field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|