TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 6 Jan 2009 14:31:36 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner engelmaier <[log in to unmask]>
Subject:
From:
Werner engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (76 lines)
 Hi Eli,
Ever heard of the 'bimetallic strip' effect?
That top-to-bottom delta-T will cause warping; that was bad enough with SnPb but has much worse effects with the EU-RoHS-mandated Pb-free solders.
The possible consequences are pad cratering, foil/resin interfacial failure, trace fracture, head-on-pillow SJs.

Werner
Future workshops:
Pb-Free Soldering Processes: Survival, Quality, Reliability—PROBLEMS & SOLUTIONS, March 3, IPC/JEDEC Santa Clara, CA
Solder Joint Reliability: Part 1—Solder Joint Reliability Fundamentals, March 29, IPC EXPO/APEX Las Vegas
Pb-Free Soldering Processes: Survival, Quality, Reliability: PROBLEMS & SOLUTIONS, March 30, IPC EXPO/APEX Las Vegas



 


 

-----Original Message-----
From: Eli Sarig <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, 6 Jan 2009 2:16 pm
Subject: [TN] Question about bottom heaters of reflow oven










Hi all,

My question is related to the necessity of down heaters in the reflow oven.
When we solder double sided boards, we *can* create a suitable reflow
profile using *only* the top heaters of the oven.
In that case, the bottom heaters remain at room temperature. We measure
almost the same temperature on top and bottom of the board.
Are there any limitations or problems that might happen using this kind of
process?

Thanks,

Eli.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field):20SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2