TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Edwards <[log in to unmask]>
Date:
Thu, 15 Jan 2009 17:26:51 +0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Tan Geok Ang <[log in to unmask]>
Subject:
From:
Tan Geok Ang <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (239 lines)
Hi Paul,

      Please refer to below:

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Thursday, 15 January 2009 11:52 AM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open

 

GA Tan...

 

A couple of questions....

Pitch and ball size of BGA --> 40mils, 19mils

PCB pad size -->16mils

PCB material and thickness --> FR4, 1.6mm

Underfill material - SunStar 991

What solder and ball metalllury --> SAC 

Top and bottom heater temps 

Time above 230C --> about 45sec

Cooldown ramp rate--> 2.8 sec

How was 16G force generated and how was the coupon mounted to the
generator --> fixture

 

 

 

 

Paul

 

Paul Edwards

Surface Art Engineering

 

 

 

-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Tan Geok Ang

Sent: Wednesday, January 14, 2009 5:27 PM

To: [log in to unmask]

Subject: [TN] Possible cause on open

 

Hi Steve,

 

            Please help to download these pictures TechNet, thanks.

 

 

 

 

 

 

 

Hi All experts,

 

            Testing (combine test of 16G at 85 oC) was performed on

evaluation boards with under-filled BGAs. Open issue (cracks) was

detected only at some corners of the BGA (35x35mm with 1156 balls) after

the test. Lead-free process and PCB with ENIG surface finish. Peak

temperature is 248 oC with a 65 sec above 217 oC.

 

FYI, the service lab has not come out a report.

 

            What are the possible causes? (CET mismatches, Lead-free

alloy related, material, processes)

 

 

 

            Thank you in advance.

 

 

 

Regards

 

GA Tan

 

 

 

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:
http://listserv.ipc.org/archives

Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815

-----------------------------------------------------

 

========================================================================
======

 

This email and any attachments thereto may contain private,
confidential, and

privileged material for the sole use of the intended recipient. Any
review, copying,

or distribution of this email (or any attachments thereto) by others is
strictly prohibited.

If you are not the intended recipient, please contact
[log in to unmask]

immediately and permanently delete the original and any copies of this
email and

any attachments thereto. 

 

========================================================================
======

 

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:
http://listserv.ipc.org/archives

Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815

-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2