A tiny "sliver" from a solder pad with EDS will give you the answer.
Vladimir
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Tremmel
Sent: Wednesday, January 14, 2009 1:15 PM
To: [log in to unmask]
Subject: Re: [TN] Discrimanting Imersion Sn from Immersion Ag on PCB's
Hello,
Crap a good board?
If I could, If I only could, I surely would (sung like Simon and
Garfunkel)
But then again I hate to think of what I would have to eat in order to
do that !!
Thank you, David Tremmel> Date: Wed, 14 Jan 2009 12:37:38 -0500> From:
[log in to unmask]> Subject: Re: [TN] Discrimanting Imersion Sn from
Immersion Ag on PCB's> To: [log in to unmask]> > As long as you don't use
it on an active pad - don't want to crap a good> board!> > Bev> RIM> >
-----Original Message-----> From: TechNet [mailto:[log in to unmask]] On
Behalf Of Gabriela> Sent: Wednesday, January 14, 2009 1:37 PM> To:
[log in to unmask]> Subject: Re: [TN] Discrimanting Imersion Sn from
Immersion Ag on PCB's> > Maybe you can try:>
http://www.koslow.com/metaltestchart.html> I don't know how sensitive
these are for thin coatings...> Gaby> -----Original Message-----> From:
TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez> Sent:
Wednesday, January 14, 2009 2:55 PM> To: [log in to unmask]> Subject: Re:
[TN] Discrimanting Imersion Sn from Immersion Ag on PCB's> > How about
XRF?> > -----Original Message-----> From: TechNet
[mailto:[log in to unmask]] On Behalf Of Larry Dzaugis> Sent: Tuesday,
January 13, 2009 5:09 PM> To: [log in to unmask]> Subject: [TN]
Discrimanting Imersion Sn from Immersion Ag on PCB's> > We have several
PCB's produced with Immersion Ag and Immersion Sn> finish.> Is there
quick test to check the finish on the PCB to determine which> finish> it
is?> > The Sn appears greyer than the Ag but the sample size is small.>
> The drawings do call out the finish, looking for a way to verify
which> was> shipped.> >
---------------------------------------------------> Technet Mail List
provided as a service by IPC using LISTSERV 15.0> To unsubscribe, send a
message to [log in to unmask] with following text> in> the BODY (NOT the
subject field): SIGNOFF Technet> To temporarily halt or (re-start)
delivery of Technet send e-mail to> [log in to unmask]: SET Technet NOMAIL
or (MAIL)> To receive ONE mailing per day of all the posts: send e-mail
to> [log in to unmask]: SET Technet Digest> Search the archives of
previous posts at:> http://listserv.ipc.org/archives> Please visit IPC
web site> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional> information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100> ext.2815>
-----------------------------------------------------> >
---------------------------------------------------> Technet Mail List
provided as a service by IPC using LISTSERV 15.0> To unsubscribe, send a
message to [log in to unmask] with following text> in> the BODY (NOT the
subject field): SIGNOFF Technet> To temporarily halt or (re-start)
delivery of Technet send e-mail to> [log in to unmask]: SET Technet NOMAIL
or (MAIL)> To receive ONE mailing per day of all the posts: send e-mail
to> [log in to unmask]: SET Technet Digest> Search the archives of
previous posts at:> http://listserv.ipc.org/archives> Please visit IPC
web site> http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for
additional information, or contact Keach Sasamori at [log in to unmask]> or>
847-615-7100 ext.2815>
-----------------------------------------------------> >
---------------------------------------------------> Technet Mail List
provided as a service by IPC using LISTSERV 15.0> To unsubscribe, send a
message to [log in to unmask] with following text> in> the BODY (NOT the
subject field): SIGNOFF Technet> To temporarily halt or (re-start)
delivery of Technet send e-mail to> [log in to unmask]: SET Technet NOMAIL
or (MAIL)> To receive ONE mailing per day of all the posts: send e-mail
to> [log in to unmask]: SET Technet Digest> Search the archives of
previous posts at:> http://listserv.ipc.org/archives> Please visit IPC
web site> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional> information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100> ext.2815>
-----------------------------------------------------> >
--------------------------------------------------------------------->
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.> >
---------------------------------------------------> Technet Mail List
provided as a service by IPC using LISTSERV 15.0> To unsubscribe, send a
message to [log in to unmask] with following text in> the BODY (NOT the
subject field): SIGNOFF Technet> To temporarily halt or (re-start)
delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
or (MAIL)> To receive ONE mailing per day of all the posts: send e-mail
to [log in to unmask]: SET Technet Digest> Search the archives of previous
posts at: http://listserv.ipc.org/archives> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|