TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 2 Jan 2009 09:21:54 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Igoshev, Vladimir" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="UTF-8"
From:
"Igoshev, Vladimir" <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
Any time Bev :-)



----- Original Message -----

From: Bev Christian <[log in to unmask]>

To: TechNet E-Mail Forum <[log in to unmask]>; Igoshev, Vladimir

Sent: Fri Jan 02 09:21:14 2009

Subject: RE: [TN] PWB Delamination Detection by C-SAM



Thanks, Vlad.

Bev



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir

Sent: Friday, January 02, 2009 9:21 AM

To: [log in to unmask]

Subject: Re: [TN] PWB Delamination Detection by C-SAM



Unless it's so thick that no signal will go through it should work. That

is why  a low frequency trancducer is used and that is why it should be

a through mode - it won't tell where (which layers) but the location

(X:Y)



Vladimir



----- Original Message -----

From: Bev Christian <[log in to unmask]>

To: TechNet E-Mail Forum <[log in to unmask]>; Igoshev, Vladimir

Sent: Fri Jan 02 09:14:24 2009

Subject: RE: [TN] PWB Delamination Detection by C-SAM



But won't it depend on how thick the board is - how many layers?  If it

is a really thick one and the delam is in the middle...

Bev



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir

Sent: Friday, January 02, 2009 9:13 AM

To: [log in to unmask]

Subject: Re: [TN] PWB Delamination Detection by C-SAM



Hi Victor,



Through scan with a low frequency (30 or 15) transducer should be able

to do it.



Regards,



Vladimir



----- Original Message -----

From: TechNet <[log in to unmask]>

To: [log in to unmask] <[log in to unmask]>

Sent: Fri Jan 02 09:09:57 2009

Subject: [TN] PWB Delamination Detection by C-SAM



Fellow TechNetters: 



   Searching for supporting information on non destructive analysis with

C-SAM to confirm raw board delamination.   



Victor,



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------





---------------------------------------------------------------------

This transmission (including any attachments) may contain confidential

information, privileged material (including material protected by the

solicitor-client or other applicable privileges), or constitute

non-public information. Any use of this information by anyone other than

the intended recipient is prohibited. If you have received this

transmission in error, please immediately reply to the sender and delete

this information from your system. Use, dissemination, distribution, or

reproduction of this transmission by unintended recipients is not

authorized and may be unlawful.





---------------------------------------------------------------------

This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.




ATOM RSS1 RSS2