TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 26 Jan 2009 09:16:33 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Creswick <[log in to unmask]>
Subject:
From:
Steven Creswick <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (117 lines)
Victor,

This is what I was referring to.  The first link is for the 5 minute gel.
The second is for the plain 5 minute version that you can buy at many home
repair or automotive parts stores.

http://www.devcon.com/prodfiles/pdfs/fam_tds_176.pdf

http://www.devcon.com/prodfiles/pdfs/fam_tds_175.pdf

They are not greatly different from what you are currently using except that
they are viscous liquids to begin with instead of putty-like.  You may find
that your current supplier also has paste-like versions

If this does not tell you what you are looking for, you can drop me a line
directly if you wish.

Steve

[log in to unmask]



On Mon, Jan 26, 2009 at 8:41 AM, <[log in to unmask]> wrote:

> Steve,
>
>   When I Google DEVCON I came across this site.
>
> http://www.devcon.com/resources/technicalInformation.cfm
>
> Did you have A PRODUCT NAME IN MIND?
>
>
> Victor,
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
> Sent: Thursday, January 22, 2009 3:12 PM
> To: [log in to unmask]
>  Subject: Re: [TN] Epoxy Putty Stick
>
> Victor,
>
> Have you tried simple old "5 minute epoxy" from Devcon?  There are many
> other similar products as well and many will do a nice job provided you
> are
> gluing an inverted top-hat down on the device to maximize adhesive
> interface
> area.
>
> Steve
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
> Sent: Thursday, January 22, 2009 4:01 PM
> To: [log in to unmask]
> Subject: [TN] Epoxy Putty Stick
>
> Fellow TechNetters:
>
>   I am currently using AquaMend, and/or Waterweld products for pull
> test on Ball Grid Arrays package and have great peel strength even on
> quarter inch square BGAs.   I'm searching for a product that does nor
> require hand mixing of a solid stick.   Any suggestions and/or comments
> will be greatly appreciated.
>
> vic,
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask]
> or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2