TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Date:
Fri, 16 Jan 2009 13:54:17 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
From:
John Burke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-2022-jp"
MIME-Version:
1.0
Parts/Attachments:
text/plain (484 lines)
There I was wanting to pee
Standing on the lectern - only me
Giving the lecture full of fear
Wishing I hadn't had that last beer.........

It's FRIDAY.............

John Burke
(408) 515 4992


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey (EHCOE)
Sent: Friday, January 16, 2009 1:34 PM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open

And to me it will bring such great glee
Cause all I ever wanted was a pot to pee
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Friday, January 16, 2009 2:28 PM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open

Gold and silver have I none,
but such as I have give I thee.. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner engelmaier
Sent: Friday, January 16, 2009 2:14 PM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open


 Dewey,
You read like the 'gold' commercial.
Au + Ag = double-whammy

Werner


 


 

-----Original Message-----
From: Lee Whiteman <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, 16 Jan 2009 2:47 pm
Subject: Re: [TN] Possible cause on open










Au + Ag → Bling (?)

Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey (EHCOE)
Sent: Friday, January 16, 2009 2:44 PM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open

Augh! You can never have too much Au, unless it's more flash than substance.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner engelmaier
Sent: Friday, January 16, 2009 12:35 PM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open


 Hi richard,
where do these PCBs come from? Not everything called ENIG is in fact
immersion Au--thus, you can have too m uch Au.

Werner
Future workshops:
Pb-Free Soldering Processes: Survival, Quality, Reliability-PROBLEMS &
SOLUTIONS, March 3, IPC/JEDEC Santa Clara, CA Solder Joint Reliability: Part
1-Solder Joint Reliability Fundamentals, March 29, IPC EXPO/APEX Las Vegas
Pb-Free Soldering Processes: Survival, Quality, Reliability: PROBLEMS &
SOLUTIONS, March 30, IPC EXPO/APEX Las Vegas



 


 

-----Original Message-----
From: Thayer, Wayne <[log in to unmask]>
To: [log in to unmask]
Sent: Fri,=2
016 Jan 2009 11:02 am
Subject: Re: [TN] Possible cause on open










 My vote says this is not ENIG--it is ENEG!

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Friday, January 16, 2009 10:48 AM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open

I expanded the images and I am sending them back to Steve for re-posting. I
can see a lot of flower-petal patterns, a lot of rod and cone structures
just above the IMC. It appears as if there are very heavy gold
intermetallics along the top of the IMC, and the gold nucleated back towards
the IMC from the solder ball. 
The IMC layer is very thin.
The solder between the edge of the soldermask and the edge of the pad causes
the pad edge to look like they curled at the edges, but I think you can see
that it is just the crack curling downwards inside of the sol der. Full
reflow obviously took place because the solder melted down the sides of the
pads and filled the space between the soldermask and the curled edges of the
pad. In the image taken near the center of the pad, it is obvious the crack
propogated through the solder in some areas.
The crack along the entire length of the pad and down the sides indicates
severe stresses due to either the vibration forces or the CTE from the
temperature cycling, or both. The crack probably formed due to the brittle
nature of the IMF, what with having the worst possible combination of ENIG ,
lead-free solder, and lateral stresses. There are some voids with flux
debris above the whole thing that tend to confuse the issues going on.
Steve, I am sending my expanded image to you for posting separately.
Thanks.
Richard

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir
Sent: Thursday, January 15, 2009 8:42 PM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open

Thank you for sending me the image. Honestly, I don't quite understand what
I see. The finish doesn't look like ENIG and the cavity above something that
DOES NOT look like a typical intermetallic shouldn't be there, not to
mention a "hair-like" something (crack?????) above the cavity.

It looks like a proper joint had never been formed. Can you ask the lab to
slightly etch the section?

Regards,

Vladimir

________________________________

From: Tan Geok Ang
To: Igoshev, Vladimir; TechNet@IP
C.ORG
Sent: Thu Jan 15 20:09:33 2009
Subject: RE: [TN] Possible cause on open


About 1.05um



________________________________

From: Igoshev, Vladimir [mailto:[log in to unmask]]
Sent: Friday, 16 January 2009 9:01 AM
To: Tan Geok Ang; [log in to unmask]
Subject: Re: [TN] Possible cause on open



The info I'm asking about is at the bottom of the images you sent to Steve.
You should be able to read from the originals what it says (how many
microns)

Regards,

Vladimir

----- Original Message -----
From: Tan Geok Ang <[log in to unmask]>
To: TechNet E-Mail Forum <[log in to unmask]>; Igoshev,  Vladimir
Sent: Thu Jan 15 19:53:13 2009
Subject: RE: [TN] Possible cause on open

The service lab has not come out much information at this time. Will input
you once I have the information. Thank you.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir
Sent: Thursday, 15 January 2009 10:50 PM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open

It looks like there could be something fishy in the intermetallic layer.
GA, can you tell me please what is the reading on the micron bars?

Regards,

Vladimir

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, January 15, 2009 8:05 AM
To: [log in to unmask]
Subject: Re: [TN] Possible cause on open

Mornin' Everbody!

Well, here in Tulsa, we're just like a lot of other people in the country
this morning, trying to stay warm. Right now we're sitting at -10 C. with a
wind chill of -15 C. It's supposed to be colder tomorrow...

GA, I have your pictures posted now. They're at:

http://stevezeva.homestead.com/files/Fracture1.jpg

http://stevezeva.homestead.com/files/Fracture2.jpg

Hopefully someone can give you some ideas...

Steve


________________________________

From: Tan Geok Ang [mailto:[log in to unmask]]
Sent: Wednesday, January 14, 2009 7:27 PM
To: [log in to unmask]; Steve Gregory
Subject: Possible cause on open



Hi Steve,

            Please help to download these pictures TechNet, thanks.







Hi All experts,

          =2
0 Testing (combine test of 16G at 85 oC) was performed on evaluation boards
with under-filled BGAs. Open issue (cracks) was detected only at some
corners of the BGA (35x35mm with 1156 balls) after the test. Lead-free
process and PCB with ENIG surface finish. Peak temperature is 248 oC with a
65 sec above
217 oC.

FYI, the service lab has not come out a report.

            What are the possible causes? (CET mismatches, Lead-free alloy
related, material, processes)



            Thank you in advance.



Regards

GA Tan




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in
the BODY 
(NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
 To receive ONE mailing per day of 
all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or 
contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in
the BODY 
(NOT the subject field):=2
0SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of 
all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or 
contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in
the BODY 
(NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) 
delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
or 
(MAIL) To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:
 SET Technet Digest Search the archives of previous posts at: 
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------

This e-mail and any files transmitted with it may be proprietary and are

intended solely for the use of the individual or entity to whom they are

addressed. If you have received this e-mail in error please notify the
sender.
Please note that any views or opinions presented in this e-mail=2
0are
solely those 
of the author and do not necessarily represent those of ITT Corporation.
The 
recipient should check this e-mail and any attachments for the presence
of 
viruses. ITT accepts no liability for any damage caused by any virus
transmitted 
by this e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-6
15-7100 ext.2815
-----------------------------------------------------



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please 
visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for 
additional information, or con
tact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2