Yes, X-outs are common. Whether an indicator of competence, it depends on the resolution/difficulty of manufacture. Generally, if there are too many x-outs, the vendor will go out of business!
By the way, we use DuPont Axarel 2200 sprayed in an air brush followed by alcohol in an airbrush followed by air in an airbrush! The alcohol alone just seems to move the flux around and won't attack the heavy deposits.
Wayne Thayer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wilson, Bob
Sent: Wednesday, December 17, 2008 1:58 PM
To: [log in to unmask]
Subject: Re: [TN] x-outs in panel
Thanks for all of the great replies on the board cleaning question....
Here's another:
Purchasing is asking: When a fabricator panels a board and there are x-outs within the panel, does that mean that the fabricator isn't competent?
We have received 90% of our boards separated into single units and we now have an assembler that wants the boards in a panel. Some of the boards in the panel are x-ed out.
I'm saying that x-outs are common enough, that more than one board is usually not good enough to be used for production, but that is because of the tight tolerances and difficult manufacturing methods.
Is that a good argument?
Bob Wilson
E/M Designer, CID+
SpectraSensors, Inc.
11027 Arrow Route
Rancho Cucamonga, CA 91730
(909) 948-4110
www.spectrasensors.com
www.ipc.org
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|