Good-day Dave,
Conductive epoxy is "sort of conductive"; it is really quite resistive. What I have noticed is that manufacturers tend to believe that it can be used instead of good plating control. The conductive epoxy contacts may be OK in a digital circuit, but they are usually unacceptable in the analog realm. I use only non-conductive epoxy and plate over the ends of the cylinders and keep a close eye on the plating of the via holes. You should only need to do this if you are designing a "via in pad" structure. If you design a dog-bone (interstitial) structure, the holes should not need to be filled if the hole to pad size ration is correct. Reference the application note at the following link for a fair discussion of PCB concerns and design reliability on fine pitch packages.
http://focus.ti.com/general/docs/techdocsabstract.tsp?abstractName=spraa99
Good designs to you,
Kim Haynes
Interface and Clock Products
High-Speed Serial Link Applications
Texas Instruments, Inc.
214-567-2057 Telephone
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Connitt
Sent: Tuesday, December 02, 2008 9:01 AM
To: [log in to unmask]
Subject: Re: [TN] Conductive Epoxy filled Vias
Joyce,
Our board house is concerned about meeting the 0.003" annular ring
requirement with a drill and hole size that small. Remember they have to
use a larger drill size to get our finished hole size. The conductive
epoxy sounds like it will "relieve us" of that issue..
Dave Connitt
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Tuesday, December 02, 2008 9:16 AM
To: [log in to unmask]
Subject: Re: [TN] Conductive Epoxy filled Vias
Why not plated via?
--------------------------
Sent using BlackBerry
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Tue Dec 02 09:07:27 2008
Subject: [TN] Conductive Epoxy filled Vias
Hello List,
We are considering implementing a 0.80 mm pitch BGA on a development
project and I have question about escape vias.
The part manufacturer recommends that we use a 0.019" pad with a 0.010"
drill. The board has to be a IPC-6012 class 3 PWB and I would like to
have a 0.003 annular ring on the escape vias.
One of our board vendors suggested we use a epoxy filled via which would
relieve us of the annular ring issue but I am not sure about still being
a class 3 board. Does anybody know where I can confirm that epoxy filled
vias are acceptable in a class 3 board?
Thanks,
Dave Connitt CID+
Printed Circuit Designer
KDI Precision Products, Inc.
A Wholly Owned Subsidiary of:
L3 Communications
3975 McMann Road
Cincinnati, Ohio 45245
Ph. 513- 943-2010 Fax 513-943-2288
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|