解决立碑,请使用熔点温度范围宽点的焊膏,一般共晶焊膏立碑概率多些。
"zhidon
g.chen"
<zhidon 收件人
g.chen@ [log in to unmask]
HOLLEY. 抄送
CN>
发件人: 主题
TGAsia [TGAsia] 关于元器件立碑问题,请教各位
<TGAsia
@ipc.or
g>
2008-12
-24
09:29
请答复
给
Asia
Committ
e Task
Group
Forum
<TGAsia
@IPC.OR
G>; 请
答复 给
"zhidon
g.chen"
<zhidon
g.chen@
HOLLEY.
CN>
各位:圣诞节好!
近期本公司更换锡膏后,发现0603器件在PCB边上,出现立碑现象增多,想请
教:立碑导致的原因,与锡膏影响大还是与温度曲线影响大?谢谢!
陈智东
2008-12-24
zhidong.chen
--------------------------------------------------------
ZTE Information Security Notice: The information contained in this mail is solely property of the sender's organization. This mail communication is confidential. Recipients named above are obligated to maintain secrecy and are not permitted to disclose the contents of this communication to others.
This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the originator of the message. Any views expressed in this message are those of the individual sender.
This message has been scanned for viruses and Spam by ZTE Anti-Spam system.