Greetings folks
Found this on the wires today... (Cut it earlier out but lost the link but I
am sure I am not the only one who read it. However I can go dig it up if
there is interest)
Why are we still using lead-free solder again? So it goes....
Joe
"Davide de Maio of National Physical Laboratory discussed the high frequency
vibration testing of tin-lead and lead-free solder joints, with reference to
automotive and aerospace electronics--a grim reminder that 80% of failures
in airborne electronics were attributable to vibration and shock. A test piece
had been designed representing a single solder joint between two copper
components, which was tested to failure at frequencies of 400Hz and 800Hz. A
range of SAC lead-free solders had been evaluated, with tin-lead as a comparison.
The tin-lead solder outperformed the lead-free examples, especially at the
higher frequency. In general, failure occurred at or near the intermetallic
interface, which would be expected to be the most stressed area. Of the SAC
alloys, performance at 400Hz was better the higher the silver content. Annealing
of SAC had a deleterious effect on performance at both 400Hz and 800Hz."
**************Make your life easier with all your friends, email, and
favorite sites in one place. Try it now.
(http://www.aol.com/?optin=new-dp&icid=aolcom40vanity&ncid=emlcntaolcom00000010)
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|