Hi,
I just received the 'Final Draft of the C-revision for PC-4101, Specification
for Base Materials for Rigid and Multilayer Printed Boards.
I am rather disappointed to find that the STII-concept has not been included
in this draft. I was promised that the concept would get serious consideration
and be included in the C-revision 'if appropriate'.
Over 2 years have passed since I withdrew my NEGATIVE on the B-revision of
this document to expedite its timely publication, even though flawed. From what
I can tell from the meeting minutes absolutely nothing has been done by the
committee regardng the inclusion of the STII-concept into IPC-4101C.
The STII-concept has found favorable interest by users both in the USA and
Europe, with some interest expressed in Asia as well. Its effectiveness is
clearly evident, it does not take anything away from any of the materials, it makes
selection for suitability much easier, and it combines the impact of the
major parameters affecting PCB survival/reliability.
Given the impact of the high LF-soldering temperatures on the survivability
and reliability of PCBs, and given the fact that more and more people are
actually going LF-free, it is important that designers are given all appropriate
and necessary tools.
As this draft stands, I will vote NEGATIVE.
However, if I am a single voice in the wilderness, the committee might be
tempted to again postpone addressing the issues. I therefore urge you send
appropriately worded comments to the people below:
[log in to unmask]
[log in to unmask]
[log in to unmask]
[log in to unmask]
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|