Also the heatsink's mass will stress the solder joints if they are not mounted to the PCB...But the biggest problem I have seen is that the heat sink hits things in transport and handling...I have also seen people use the heatsinks used as handles on PCAs...
The other possibility is that the BGA balls may have an adhesion problem with the BGA substrate... This should be observable when the BGA is removed.
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner engelmaier
Sent: Thursday, December 04, 2008 8:14 PM
To: [log in to unmask]
Subject: Re: [TN] 答复: Re: [TN] BGA soldering open issue
Nee hao Hechong,
BGAs with heatsinks have been shown to warp and thus loading the SJs in tension.
Werner
-----Original Message-----
From: Cong He <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, 4 Dec 2008 10:08 pm
Subject: [TN] 答复: Re: [TN] BGA soldering open issue
surface finish is hasl.
after analysed parts of the board, we found some balls of the bga rupture.
Could it be the material of the ball(BGA) cause the problem?
by the way, there is a heatsink which is double size lager than the chip
stick on it without other fixture.
will the heatsink be the reason?
Hechong
"Wenger, George M." <[log in to unmask]>
发件人: TechNet <[log in to unmask]>
2008-12-05 10:57
请答复 给
TechNet E-Mail Forum <[log in to unmask]>; 请答复 给
"Wenger, George M." <[log in to unmask]>
收件人
[log in to unmask]
抄送
主题
Re: [TN] BGA soldering open issue
What is the surface finish on your PCBA?
Necong,
What is the surface finish on your PCBA?
Regards,
George
George M. Wenger
Andrew Wireless Solutions
Senior Principal FMA / Reliability Engineer
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [Office] (732) 309-8964 [Cell]
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cong He
Sent: Thursday, December 04, 2008 9:09 PM
To: [log in to unmask]
Subject: [TN] BGA soldering ope
n issue
dear all:
I am facing a problem of bga soldering.
when the board have just soldered ,it pass all test.
But after sometime, maybe for a few weeks,
some of the bga balls opened. the function became normal if i press the
chip on the top side.
It seems that the pcb didn't warp much,it seems even no warp at all.
Does any of you know why? And how to improve?
Hechong
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
No virus found in this incoming message.
Checked by AVG - http://www.avg.com
Version: 8.0.176 / Virus Database: 270.9.13/1828 - Release Date:
12/4/2008 8:05 AM
------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notif
y the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
==============================================================================
This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review, copying,
or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto.
==============================================================================
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|