Phil,
Have seen the same problem with Henkel material...
But the underfill appears to harden or semi-cure over time (after 2-3 wks) ....
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phillip Bavaro
Sent: Monday, December 22, 2008 3:02 PM
To: [log in to unmask]
Subject: [TN] Underfill, inhibition due to leftover activators in the flux residue
I have made quite a few test samples and discovered that a certain
underfill material will exhibit inhibited cure when it comes in contact
with solderpaste flux residues at the center of a very dense BGA component.
The rest of the underfill beneath the BGA will harden like normal.
We don't clean nor plan on starting to clean our assemblies.
DVT testing does not show any defects due to underfill adhesion.
Background:
We used a four up ABAB panel which goes through SMT twice.
BGAs only passing through the oven once consistently show the problem.
Two passes through the reflow oven (ABAB flip) and the problem goes away.
This means that half of our test samples still have soft material in the
pocket at the center where the power ground pins are located.
We measure peak temperature in this area and have found that raising the
peak temperature helps quite a bit but does not eliminate the inhibition
entirely.
The manufacturers of the paste and the underfill acknowledge the issue but
do not have a solution.
Has anyone else run into similar compatibility issues with a paste and
underfill?
In the event that we cannot work out the root cause, and decide to make a
change, I am trying to come up with a list of all the manufacturers of
underfill.
So far I have found 8 major underfill manufacturers but would appreciate
knowing about more if there are any.
3M
Ablestik
Epotek
Henkel
Hysol
SP&S
Sunstar
Zymet
Thanks in advance,
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
==============================================================================
This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review, copying,
or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto.
==============================================================================
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|