TECHNET Archives

December 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Sun, 7 Dec 2008 15:18:52 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain
From:
John Goulet <[log in to unmask]>
Parts/Attachments:
text/plain (148 lines)
I would hope your using an underfill material to prevent the shear stresses when a large heat sink is used.

-------------- Original message -------------- 
From: Cong He <[log in to unmask]> 

> surface finish is hasl. 
> 
> after analysed parts of the board, we found some balls of the bga rupture. 
> Could it be the material of the ball(BGA) cause the problem? 
> 
> by the way, there is a heatsink which is double size lager than the chip 
> stick on it without other fixture. 
> will the heatsink be the reason? 
> 
> 
> 
> 
> 
> 
> Hechong 
> 
> 
> 
> 
> 
> "Wenger, George M." 
> 发件人: TechNet 
> 2008-12-05 10:57 
> 请答复 给 
> TechNet E-Mail Forum ; 请答复 给 
> "Wenger, George M." 
> 
> 
> 收件人 
> [log in to unmask] 
> 抄送 
> 
> 主题 
> Re: [TN] BGA soldering open issue 
> 
> 
> 
> 
> 
> 
> What is the surface finish on your PCBA? 
> 
> 
> 
> Necong, 
> 
> What is the surface finish on your PCBA? 
> 
> Regards, 
> George 
> George M. Wenger 
> Andrew Wireless Solutions 
> Senior Principal FMA / Reliability Engineer 
> 40 Technology Drive, Warren, NJ 07059 
> (908) 546-4531 [Office] (732) 309-8964 [Cell] 
> [log in to unmask] 
> 
> 
> -----Original Message----- 
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Cong He 
> Sent: Thursday, December 04, 2008 9:09 PM 
> To: [log in to unmask] 
> Subject: [TN] BGA soldering open issue 
> 
> dear all: 
> 
> I am facing a problem of bga soldering. 
> 
> when the board have just soldered ,it pass all test. 
> But after sometime, maybe for a few weeks, 
> some of the bga balls opened. the function became normal if i press the 
> chip on the top side. 
> 
> It seems that the pcb didn't warp much,it seems even no warp at all. 
> Does any of you know why? And how to improve? 
> 
> 
> 
> 
> 
> 
> Hechong 
> 
> --------------------------------------------------- 
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 
> To unsubscribe, send a message to [log in to unmask] with following text 
> in 
> the BODY (NOT the subject field): SIGNOFF Technet 
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL) 
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest 
> Search the archives of previous posts at: 
> http://listserv.ipc.org/archives 
> Please visit IPC web site 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
> ext.2815 
> ----------------------------------------------------- 
> 
> 
> No virus found in this incoming message. 
> Checked by AVG - http://www.avg.com 
> Version: 8.0.176 / Virus Database: 270.9.13/1828 - Release Date: 
> 12/4/2008 8:05 AM 
> -------------------------------------------------------------------------------- 
> ---------------- 
> This message is for the designated recipient only and may 
> contain privileged, proprietary, or otherwise private information. 
> If you have received it in error, please notify the sender 
> immediately and delete the original. Any unauthorized use of 
> this email is prohibited. 
> -------------------------------------------------------------------------------- 
> ---------------- 
> [mf2] 
> 
> 
> --------------------------------------------------- 
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 
> To unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet 
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL) 
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest 
> Search the archives of previous posts at: http://listserv.ipc.org/archives 
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815 
> ----------------------------------------------------- 
> 
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2