Hi Rudolph,
Sounds like you have a failure that only shows up under certain conditions---this could include fractured vias, pad cratering with trace fracture, pillow-on-head, brittle interfacial failures, etc.
You might try to test the assembly at elevated T [say 50C], or while slightly bending or vibrating it.
Werner
-----Original Message-----
From: Rudolph yu <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, 22 Dec 2008 1:34 pm
Subject: [TN] What could be the root cause for a failed board that passed functiona test after going through reflow for the 2nd time?
Hi:
We have a proto assembly that passed the functional test initially. But after
we shipped it to the customer, it failed at the their site for the same kind of
test. After we received the board back, we reflowed it using the same reflow
profile, and the board would funcation once again...
We checked the boards under 5DX after we received it back from the customer and
found no defects on it.
What could be causing this? and why the assembly would pass the test in the
first place?
Here iare couple areas that I could think of...but not sure if they are valid.
1. Certain parts (microBGA) may be better off to have underfill underneath for
thermal mismatch? ( Need to check spec)
2. During handling and shipping, the board may be stressed to a degree that a
microfacture is formed.
What other areas could cause this problem.
Thanks
Rudolph
_________________________________________________________________
Life on your PC is safer, easier, and more enjoyable with Windows Vista®.
http://clk.atdmt.com/MRT/go/127032870/direct/01/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|