I need to remove multiple broad areas of solder mask to expose ground plane on populated boards as a result of a layout fubar. Laser removal appears to be the least risky and doesn't require masking, corrosive chemicals, or deftness with an X-Acto or Dremel tool. Does anyone have experience with this removal method? Recommended or non-recommended suppliers?