If you do run into Ron buy him too beers and I'll pay for
Steve,
If you do run into Ron buy him too beers and I'll pay for yours and his.
Great dendrite images. I've seen silver dendrites grow off a silver
plated die paddle before but not off a die bond pad.
Regards,
George
George M. Wenger
Andrew Wireless Solutions
Senior Principal FMA / Reliability Engineer
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [Office] (732) 309-8964 [Cell]
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, November 07, 2008 2:51 PM
To: [log in to unmask]
Subject: [TN] DENDRITE GROWTH
Hi Jon!
Got your pictures posted. Go to:
http://stevezeva.homestead.com/files/Dendrites_1.jpg
http://stevezeva.homestead.com/files/Dendrites_2.jpg
http://stevezeva.homestead.com/files/Dendrites_3.jpg
Really nice photos of dendrites, beautiful fern-like structure.
Maybe one day we'll run into each and you can buy me that beer, but only
if I can buy you one too...
Steve
________________________________
From: Roberts, Jon [mailto:[log in to unmask]]
Sent: Friday, November 07, 2008 12:58 PM
To: Steve Gregory
Subject: DENDRITE GROWTH
Steve, I was told you could post my pictures concerning the Dendrite
Growth inside of plastic ICs. I have enclosed the pictures two ways, in
the email body and on a .doc. The information related to this I sent
out to the TechNet group this week. Thanks in advance I was told if I
see you to buy you a beer, Jon
Enclosed is pictures of the dendrites.
Here is what the report stated associated with the pictures.
EDX Spectra #1 is from the thick part of the dendrite on the bond pad
area, and shows a strong peak of silver (Ag) along with smaller peaks of
gold (Au), copper (Cu). EDX Spectra #2 is the dendrite growth on the
Si surface; here the stronger peak is Ag with a trace of Cu. The wire
ball is seen in EDX Spectra #3 and is primarily Au with smaller traces
of Ag.
This communication is intended only for use by the addressee(s) named
herein and may contain business confidential and/or legally privileged
information. If you are not the intended recipient of this e-mail, you
are hereby notified that any dissemination, distribution, disclosure or
copying of this e-mail and its contents is strictly prohibited. If you
have received this e-mail in error, kindly notify the sender by replying
to this message. In addition, please permanently delete the message and
any attachments without copying or disclosing the contents. Thank you
for your cooperation.
THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR
TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE
EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE
APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR
DEPARTMENT OF COMMERCE.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
No virus found in this incoming message.
Checked by AVG - http://www.avg.com
Version: 8.0.175 / Virus Database: 270.9.0/1773 - Release Date:
11/7/2008 9:08 AM
------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|