Dear TN experts,
We encounter difficulty with peeling off solder mask
after vertical immersion tin. Specially, I should tell that the solder
mask thickness is enough to stand 5 times solderability test and with no
solder mask peeling off. Please kindly help give me some advises on it
to resolve.
Many thanks in advance.
Regards!
LZ