Hi Henry,
If you have any images you want to share, send them to me and I'll post
them.
Steve
----- Original Message -----
From: "henry rekers" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, November 26, 2008 6:17 PM
Subject: [TN] nickel erosion
Any technetters out there experiencing this mysterious nickel erosion
process with enig boards on their leadfree waves? Apparently there is a
committee set up already. I would like to share experiences if anyone is
willing to come forward.
Essentially, the defect shows up as a dewet on the annular ring of the TH
devices. On cross section, there is large amounts of nickel eroded away and
the surface is non-wettable. No corrosion is evident, so it's NOT black pad.
Anybody?
__________________________________________________________________
Instant Messaging, free SMS, sharing photos and more... Try the new Yahoo!
Canada Messenger at http://ca.beta.messenger.yahoo.com/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|