Hello Krishnan,
Thank you so much for your input.
Yeah, tons of our thin backplane are built with HASL. As you know, the
Lead Free HASL process has thermal shock on pcb board greater than HASL
process. We haven't built any backplanes with lead free HASL before, so we
want be sure of the reliability before making any decision. Delamination
concern? Thanks.
Best Regards
Charming Chan
PCBA Engineer
"Chezhian, Krishnan (Radhakrishnan)" <[log in to unmask]>
2008-11-04 13:57
收件人: <[log in to unmask]>
抄送:
主题: RE: [TN] Build backplane with lead free HASL surface
finish?
Hi Charming,
As long as the board thickness is below 5.0mm you should not have any
problem in running the boards through the HASL process. However the reason
we limit to 5.0mm is because the HASL process is a very harsh process
especially Lead Free HASL, this would degrade the board & also cause
fractures within the board which may not be visible to the naked eye. But
in your case the below mentioned board thicknesses should not be a concern
in running through the HASL process, we do a lot of boards upto 5.0mm……
Thanks & Best Regards,
Krishnan C
Director Of Quality
Sanmina-SCI Corporation (M) Sdn. Bhd.
Sama Jaya Free Industrial Zone
93450 Kuching, Sarawak, Malaysia.
Tel: 60 82 363 000 Ext 1602
Mobile: (6) - 012-8888-379
Fax: 60 82 363 527
E-mail: [log in to unmask]
"It is easier to do a job right than to explain why you didn't."
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, November 04, 2008 12:07 PM
To: TechNet E-Mail Forum; Chezhian, Krishnan (Radhakrishnan)
Cc: [log in to unmask]
Subject: Re: [TN] Build backplane with lead free HASL surface finish?
Hello Krishnan,
Two backplanes, the thickness and size as follows, thank you so much.
1. 2.8mm board thickness, 685mm×275.5mm board size
2. 3.2mm board thickness, 710.5mm×435mm board size
Best Regards
Charming Chan
PCBA Engineer
"Chezhian, Krishnan (Radhakrishnan)" <[log in to unmask]>
发件人: TechNet <[log in to unmask]>
2008-11-04 11:15
请答复 给 TechNet E-Mail Forum; 请答复 给 "Chezhian, Krishnan
(Radhakrishnan)"
收件人: [log in to unmask]
抄送:
主题: Re: [TN] Build backplane with lead free HASL surface
finish?
Hi Charming,
What is the thickness of the backplane??
Thanks & Best Regards,
Krishnan C
Sanmina-SCI Corporation (M) Sdn. Bhd.
"It is easier to do a job right than to explain why you didn't."
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charming Chan
Sent: Tuesday, November 04, 2008 10:45 AM
To: [log in to unmask]
Subject: [TN] Build backplane with lead free HASL surface finish?
Hello TechNet experts,
On our master fabrication drawing, the surface finish for backplane is
specified as ENIG, but the fabrication shop ask for waiver to build with
lead free HASL. Is it reliable enough? Any other concerns should be
taken
into consideration? Thanks a lot.
Best Regards
Charming Chan
PCBA Engineer
--------------------------------------------------------
ZTE Information Security Notice: The information contained in this mail
is solely property of the sender's organization. This mail communication
is confidential. Recipients named above are obligated to maintain
secrecy and are not permitted to disclose the contents of this
communication to others.
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this email in error please notify the
originator of the message. Any views expressed in this message are those
of the individual sender.
This message has been scanned for viruses and Spam by ZTE Anti-Spam
system.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for use
by the addressee(s) named herein and may contain legally privileged and/or
confidential information. If you are not the intended recipient of this
e-mail message, you are hereby notified that any dissemination,
distribution or copying of this e-mail message, and any attachments
thereto, is strictly prohibited. If you have received this e-mail message
in error, please immediately notify the sender and permanently delete the
original and any copies of this email and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS
NOT INTENDED AS A SUBSTITUTE FOR A WRITING. Notwithstanding the Uniform
Electronic Transactions Act or the applicability of any other law of
similar substance and effect, absent an express statement to the contrary
hereinabove, this e-mail message its contents, and any attachments hereto
are not intended to represent an offer or acceptance to enter into a
contract and are not otherwise intended to bind the sender, Sanmina-SCI
Corporation (or any of its subsidiaries), or any other person or entity.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
--------------------------------------------------------
ZTE Information Security Notice: The information contained in this mail is
solely property of the sender's organization. This mail communication is
confidential. Recipients named above are obligated to maintain secrecy and
are not permitted to disclose the contents of this communication to
others.
This email and any files transmitted with it are confidential and intended
solely for the use of the individual or entity to whom they are addressed.
If you have received this email in error please notify the originator of
the message. Any views expressed in this message are those of the
individual sender.
This message has been scanned for viruses and Spam by ZTE Anti-Spam
system.
CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for use
by the addressee(s) named herein and may contain legally privileged and/or
confidential information. If you are not the intended recipient of this
e-mail message, you are hereby notified that any dissemination,
distribution or copying of this e-mail message, and any attachments
thereto, is strictly prohibited. If you have received this e-mail message
in error, please immediately notify the sender and permanently delete the
original and any copies of this email and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS
NOT INTENDED AS A SUBSTITUTE FOR A WRITING. Notwithstanding the Uniform
Electronic Transactions Act or the applicability of any other law of
similar substance and effect, absent an express statement to the contrary
hereinabove, this e-mail message its contents, and any attachments hereto
are not intended to represent an offer or acceptance to enter into a
contract and are not otherwise intended to bind the sender, Sanmina-SCI
Corporation (or any of its subsidiaries), or any other person or entity.
--------------------------------------------------------
ZTE Information Security Notice: The information contained in this mail is solely property of the sender's organization. This mail communication is confidential. Recipients named above are obligated to maintain secrecy and are not permitted to disclose the contents of this communication to others.
This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the originator of the message. Any views expressed in this message are those of the individual sender.
This message has been scanned for viruses and Spam by ZTE Anti-Spam system.
|