TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 6 Nov 2008 11:36:40 EST
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Joe Fjelstad <[log in to unmask]>
Parts/Attachments:
text/plain (105 lines)
LOL My grand kids would appreciate that one Dewey
 
Cheers, 
Joe
 
 
 
In a message dated 11/6/2008 5:45:31 A.M. Pacific Standard Time,  
[log in to unmask] writes:






Subject: Re: [TN] AL CU DENDRTIES INSIDE PLASTIC  IC



Purple plague is an intermetallic alloy that is formed at  the junction

of the Aluminum pad where the Gold bondwire is  bonded.  But this is not

a dendrite, it is a  "Barny"cle.

Dewey





It is a  multi-crystalline growth that appears as a dark or

purple ring around  the ball of the gold bondwire.  Typically dendrites,

which will  grow within a contaminated plastic IC, do not contain gold.

All it  takes is the aluminum, moisture, and an electric field.



In the  past purple plague has been generally caused by high  temperature

whether or not the IC is powered.  It usually causes  an open circuit

(eventually) due to Kirkendahl voiding at the  interface.  With today's

very closely pitched bonding pads the  purple plague growth may be able

to bridge between two adjacent bonding  pads. 



But again, this is not a dendrite.  Dendrites need  an electric field to

induce growth, purple plague occurs in the absence  of an electric field.

It occurs at some rate continuously, but at  normal operating

temperatures grows so slowly that it is not considered  a primary factor

in calculating the lifetime of an IC.  



mark



Mark Woolley

PTRL  Laboratory

Avaya,  1300 West 120th Ave,   Area 33,   Westminster, CO,  8023


---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------

**************AOL Search: Your one stop for directions, recipes and all other 
Holiday needs. Search Now. 
(http://pr.atwola.com/promoclk/100000075x1212792382x1200798498/aol?redir=http://searchblog.aol.com/2008/11/04/happy-holidays-from
-aol-search/?ncid=emlcntussear00000001)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2