Obviously some water wash pastes clean off more completely than others, but
you can not assume that all wash additives improve cleaning of all fluxes.
Some water wash fluxes will clean worse - not better - if inappropriate wash
additives are used.
= make sure your proposed cleaner supplier has documented trials of his
various solutions with your candidate paste/flux type.
You will need strong procedures to make sure that you don't mix paste types
(and associated flux core solder wire, repair fluxes etc) with types from
adjacent lines. Unwashed water sol flux is not good, but water washed no
clean can also be bad news.
You will have to make sure the design is suited to water washing: no water
traps, capillary opportunities, all components suited etc. or you will see
them back just as quickly as if using the wrong materials!
Regards
Mike Fenner
Indium Corporation
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Peck
Sent: Thursday, November 20, 2008 2:07 AM
To: [log in to unmask]
Subject: Re: [TN] WS solder paste
Ioan:
I'd like to reinforce Doug Pauls' comment on cleaning water
soluble?residues.
From?a rework perspective, please don't even let?water soluble flux into the
rework area unless the the PCBs can be power-washed after rework. Have seen
some awful field returns reworked with water soluble flux that might have
been hand-cleaned, at best.
Good luck.
Doug Peck
-----Original Message-----
From: Douglas O. Pauls <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, 19 Nov 2008 11:21 am
Subject: Re: [TN] WS solder paste
Ioan,
In addition to the other suggestions given so far, do not EVER EVER EVER
believe the salesman when they tell you that water soluble flux can be
cleaned using water alone. It can't. And if they tell you that tap water
cleaning works fine, throw them out the door.
Most of the cleaning chemical vendors, such as Kyzen, Petroferm, Zestron,
can give you good data on what materials work best to ensure cleaning
under low standoff parts.
Doug Pauls
Rockwell Collins
Ioan Tempea <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
11/18/2008 09:44 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ioan Tempea <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] WS solder paste
Dear Technos,
After having worked for years with no-clean pastes, I need now to
evaluate water soluble. Concerning both SnPb and lead-free, what would
be your short list to start qualifications?
We are a CEM, so the paste needs to be very versatile, so it can give
the best performance (compromise) for inconsistent designs. In this
world we need to print everyday a wide range of designs like 20mil fine
pitch pads with widths from 9 to 15 mils, 0603s with pad gaps between 20
and 35 mils, etc., so I guess most of you understand what I mean by
versatile ;-)
I assume off-line answers would be appropriate, so please do not
hesitate...
Thank you,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional informat
ion, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|