TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sun, 9 Nov 2008 15:59:07 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain
From:
John Goulet <[log in to unmask]>
Parts/Attachments:
text/plain (15 lines)
The difference is that the leads are not coated with tin lead solder. Many components are paladium, nickle, berilium copper, gold and Sac305 so they can be used in RoHs 5 boards where you have compliance to 5 of the 6 banned elements.
The part itself may not be Pb Free but is RoHs compliant. Some lead may be needed inside the part to make it work.
Note from a process point the PCV coatings on electrolytic caps and the PET plastic used to make slide switches and low temperature plastic on the headers can present issues when you go to the high temperature lead free soldering processes in the factory. Special steps are needed to make these work.
As a manufacturing engineer I've  contacted some of the vendors on these isssues because they haven't. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2