TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob METCALF <[log in to unmask]>
Date:
Fri, 7 Nov 2008 14:00:49 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Robin John <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Robin John <[log in to unmask]>
Parts/Attachments:
text/plain (296 lines)
Thanks for that insight. So I believe the most common component finishes
for lead free are NiPdAu and matte Sn. Is that right?
Robin John
 
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob METCALF
Sent: Friday, November 07, 2008 9:20 AM
To: [log in to unmask]
Subject: Re: [TN] Build backplane with lead free HASL surface finish?

This is true with some Ni Pd Au systems as has been reported to me by
some 
military end customers. However not all systems are incompatible with 
SnPb. You should check with your fabricators chemical supplier for
details 
on their compatibility.

Regards,

Bob Metcalf
Atotech Western Regional Manager

Cell 714-334-7667
E-Mail [log in to unmask] 

This e-mail and any attachments hereto are business documents of Atotech

USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS
INFORMATION. 
Unauthorized disclosure and/or use of information contained in this
email 
is prohibited. If you are not the intended recipient, you may not read, 
use, disseminate or copy this message or any other files transmitted
with 
it. 



Grunde Gjertsen <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
11/07/2008 01:26 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] Build backplane with lead free HASL surface finish?






Wetting and intermetallic strength. My impression is that Palladium
needs 
an elevated temperature to solder well as it works fine at leadfree 
temperatures but not SnPb.
This was also a big issue with Pd plated passives some years ago but I 
don't know if it's directly comparable.

Best regards
Grunde







Bob METCALF <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
06.11.2008 03:04
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bob METCALF <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Build backplane with lead free HASL surface finish?






What sort of trouble?

Regards,

Bob Metcalf
Atotech Western Regional Manager

Cell 714-334-7667
E-Mail [log in to unmask] 

This e-mail and any attachments hereto are business documents of Atotech

USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS
INFORMATION. 


Unauthorized disclosure and/or use of information contained in this
email 
is prohibited. If you are not the intended recipient, you may not read, 
use, disseminate or copy this message or any other files transmitted
with 
it. 



Grunde Gjertsen <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
11/05/2008 05:48 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] Build backplane with lead free HASL surface finish?






You may get into trouble with ENIPIG.

Grunde






Robin John <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
04.11.2008 21:02
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Robin John <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Build backplane with lead free HASL surface finish?






Dear Experts,
What are the different RoHS component lead finishes? Will any RoHS
component lead finishes have solderability issues if used with a leaded
paste?
Thanks in advance.
Robin John
TouchSensor Technologies
e-mail: [log in to unmask]
 
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 



for additional information, or contact Keach Sasamori at [log in to unmask]
or 



847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 


for additional information, or contact Keach Sasamori at [log in to unmask]
or 


847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 

for additional information, or contact Keach Sasamori at [log in to unmask]
or 

847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2