Hi Henry! Wow, nickel plating is commonly used as a barrier layer in a
number of electronics applications so having an erosion issue would be
somewhat odd. I would expect that a lead-free soldering process would
remove more nickel (either thru erosion or dissolution) in comparison to a
tin/lead soldering process due to the increased process temperatures but
what you are describing (large?) sounds strange. Have you compared the
nickel thickness pre and post soldering process? Do you have any
microsection photos Steve could post so we could get a look at the
situation? I have run a significant number of ENIG pwbs thru both
lead-free wave and reflow processes but have not seen the condition you
describe. Are you on a mini-wave, selective solder or typical wave solder
system?
Dave Hillman
Rockwell Collins
[log in to unmask]
henry rekers <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
11/26/2008 06:17 PM
Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] nickel erosion
Any technetters out there experiencing this mysterious nickel erosion
process with enig boards on their leadfree waves? Apparently there is a
committee set up already. I would like to share experiences if anyone is
willing to come forward.
Essentially, the defect shows up as a dewet on the annular ring of the TH
devices. On cross section, there is large amounts of nickel eroded away
and the surface is non-wettable. No corrosion is evident, so it's NOT
black pad.
Anybody?
__________________________________________________________________
Instant Messaging, free SMS, sharing photos and more... Try the new Yahoo!
Canada Messenger at http://ca.beta.messenger.yahoo.com/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|