TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 21 Nov 2008 08:13:23 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Werner Engelmaier /* <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Content-Transfer-Encoding:
7bit
MIME-Version:
1.0
Parts/Attachments:
text/plain (156 lines)
 I am totally with you George.

Werner


 


 

-----Original Message-----
From: Wenger, George M. <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, 21 Nov 2008 8:00 am
Subject: Re: [TN] black pad











Ingemar is correct.  A good working relationship with your board supplier 
including continuous interactions and frequent inspection visits to insure they 
are continuing to apply appropriate process controls should help prevent many of 
the ENIG problems. However, if you follow TN closely you can see a trend that 
ENIG problems are not going away.  They continue to cause problems for many 
companies.  I believe that the primary reason for this is that most board 
suppliers today are not next door to where you are doing assembly and it is 
extremely costly in today's economy to have employees traveling (sometimes half 
a world away) to check up on suppliers.  Also in a lot of cases your board 
supplier may actually not be building your boards but may have out sourced to a 
cheaper supplier which is making it much more difficult to have confidence in 
the board fabrication process control.

One alternative is to switch to a surface finish that has less inherent problems 
and doesn't require as much process control.

Regards,
George
George M. Wenger
Andrew Wireless Solutions
Senior Principal FMA / Reliability Engineer
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [Office]  (732) 309-8964 [Cell]
[log in to unmask]
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Friday, November 21, 2008 2:49 AM
To: [log in to unmask]
Subject: Re: [TN] black pad

If you have a contiguos cooperation with your board supplier, i.e. frequent 
visits to an inspections at their plant, I think you will not see much ENIG 
problems. It's very much about good process continuity. I've said it before: we 
have assembled millions of ENIG board without problems. We had some issues many 
years ago, learned about the process and set up a cooperation model. If ENIG was 
that bad, we had changed to something else, but it wasn't necessary.
Inge 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of henry rekers
Sent: den 20 november 2008 18:46
To: [log in to unmask]
Subject: [TN] black pad

Anybody out there experiencing mass dewetting issues from North American board 
shops?
?
From what I understand primary causes for dewetting (assuming the reflow/wave 
profile is bang on) is all on the board, ie nickel corrosion, degeneration of 
the nickel, or outgassing of the nickel/copper.? (I'm talking enig here.)
?
Anybody?


      __________________________________________________________________
Connect with friends from any web browser - no download required. Try the new 
Yahoo! Canada Messenger for the Web BETA at http://ca.messenger.yahoo.com/webmessengerpromo.php

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in the BODY 
(NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) 
delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or 
(MAIL) To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest Search the archives of previous posts at: 
http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


No virus found in this incoming message.
Checked by AVG - http://www.avg.com 
Version: 8.0.175 / Virus Database: 270.9.8/1801 - Release Date: 11/20/2008 7:28 
PM
------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2