TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Jeremias, Michael" <[log in to unmask]>
Date:
Tue, 4 Nov 2008 03:07:13 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain
From:
John Goulet <[log in to unmask]>
Parts/Attachments:
text/plain (120 lines)
Thanks for the table.

-------------- Original message -------------- 
From: "Jeremias, Michael" <[log in to unmask]> 

> This table seems very valuable. 
> Pete , can You add additional information? 
> 
> Which board thicknesses are investigated? 
> Which finishes are investigated? 
> 
> I attach the information of the SMTA-Paper, reporting some investigations on 
> OSP-finish : 
> 
> IMPROVING HOLE-FILL IN LEAD-FREE SOLDERING OF THICK PRINTED CIRCUIT BOARDS WITH 
> OSP FINISH 
> Sanmina-SCI Corporation (LF2) 
> from SMTA Conference 2008, Orlando, Florida, August 17 -21, 2008 
> 
> 
> They told that they had a big rejection rate with OSP finish, where gap is 
> less than 11,5 mils. This leads to different values to Your table?. 
> 
> Sincerly 
> 
> Michael Jeremias 
> Industrial Engineering (OPPI41) 
> Electronics Production 
> ((( Defence Electronics 
> EADS Deutschland GmbH 
> 89077 Ulm 
> Tel.: +49 (0) 7 31.3 92-5533 
> Fax: +49 (0) 7 31.3 92-73 15 
> E-Fax: +49 (0) 7 31.3 92-20 5533 
> 
> mailto: [log in to unmask] 
> EADS Deutschland GmbH 
> Registered Office: Ottobrunn 
> District Court of Munich HRB 107 648 
> Chairman of the Supervisory Board: Dr. Thomas Enders 
> Managing Directors: Dr. Stefan Zoller (chairman), Michael Hecht 
> This E-mail and any attachment(s) to it are for the addressee's use only. 
> It is strictly confidential and may contain legally privileged information. No 
> confidentiality or privilege is waived or lost by any mistransmission. 
> If you are not the intended addressee, then please delete it from your system 
> and notify the sender immediateley. You are hereby notified that any use, 
> disclosure, copying or any action taken in reliance on it is strictly prohibited 
> and may be unlawful. - Thank you. 
> 
> 
> 
> -----Ursprüngliche Nachricht----- 
> Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Pete Houwen 
> Gesendet: Mittwoch, 29. Oktober 2008 14:07 
> An: [log in to unmask] 
> Betreff: Re: [TN] How to improve solder filling and wetting contact angles for 
> thermal vias at wave soldering process. 
> 
> We did some testing of design parameters when we switched to lead-free, and 
> found that the lead-hole ratio is more critical. We also found that top side 
> pad size is irrelevant for hole fill, but large bottom side pads can adversly 
> affect hole fill. Using this chart, we are able to achieve 75% with regularity 
> (and we do not have the best process controls in our plant): 
> 
> Lead Range Pad Size Hole Size 
> .000-.017 0.05 0.026 
> .018-.022 0.06 0.035 
> .023-.027 0.07 0.04 
> .028-.032 0.07 0.046 
> .033-.042 0.08 0.052 
> .043-.052 0.09 0.062 
> .053-.063 0.1 0.073 
> .064-.076 0.11 0.086 
> .077-.086 0.12 0.096 
> .087-.106 0.14 0.116 
> .107-.115 0.15 0.125 
> (dimensions in inches) 
> 
> standard plane connects are thermal relief, using (4) .008" spokes. 
> 
> This testing was done only to establish design parameters, there are plenty of 
> process parameters that will affect hole fill. But if your design parameters 
> aren't good, all the process tweaks in the world won't fix trhe problem. 
> 
> --------------------------------------------------- 
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in the BODY 
> (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) 
> delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or 
> (MAIL) To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest Search the archives of previous posts at: 
> http://listserv.ipc.org/archives Please visit IPC web site 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or 
> contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 
> ----------------------------------------------------- 
> 
> --------------------------------------------------- 
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 
> To unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet 
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL) 
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest 
> Search the archives of previous posts at: http://listserv.ipc.org/archives 
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
> additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815 
> ----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2