TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 20 Nov 2008 14:45:22 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, kwood716 <[log in to unmask]>
Subject:
From:
kwood716 <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (210 lines)
I mean copper :)
Ken

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of kwood716
Sent: Thursday, November 20, 2008 2:42 PM
To: [log in to unmask]
Subject: Re: [TN] MELF pad shape question

Hi,
You have to add a small square pad and then add the rest of the shape in
cooper.
Then associate the shape to the pad...
Ken

_____________________________________
Kenneth J. Wood
Saturn PCB Design, Inc.              [log in to unmask]
2737 Bishop Lane                       Phone:(407) 340-2668
Deltona, Fl 32725                        Fax: (386) 789-2765
www.saturnpcb.com








-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carl VanWormer
Sent: Thursday, November 20, 2008 1:58 PM
To: [log in to unmask]
Subject: Re: [TN] MELF pad shape question

Yes, we are using PADS. Any suggestions would be appreciated.

Thanks,
Carl
 




Carl Van Wormer, P.E.
Senior Hardware Engineer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR  97006
Cipher Systems (503) 617-7447   
Direct Line (503) 425-5163



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wilson, Bob
Sent: Thursday, November 20, 2008 9:13 AM
To: [log in to unmask]
Subject: Re: [TN] MELF pad shape question

Are you using PADS as a layout tool?

 

If you are, I can tell you how to do the odd pad size.

 

Bob Wilson

E/M Designer, CID+

SpectraSensors, Inc.

11027 Arrow Route

Rancho Cucamonga, CA 91730

(909) 948-4110

www.spectrasensors.com

www.ipc.org <http://www.ipc.org/> 

 

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: Thursday, November 20, 2008 7:26 AM
To: [log in to unmask]
Subject: Re: [TN] MELF pad shape question

 

Carl,

 

This notch is used to prevent edge overhang of the component. The pad

shape helps keep the component centered on the pad, otherwise the wider

middle of the component may overhang the pad edge even if the narrower

bottom is on the pad and soldered.

 

Ben

 

-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Carl VanWormer

Sent: Thursday, November 20, 2008 10:09 AM

To: [log in to unmask]

Subject: [TN] MELF pad shape question

 

A customer is using MELF parts on an existing board and is asking us to

add some more parts of a different size.  The new parts are DL-35 and

the manufacturers data sheet shows a rectangular pad as the recommended

size.  All of the MELF parts on their current board have small notches

at the middle-inside of each pad like:

 

**********                **********

**********                **********

*****                          *****

**********                **********

**********                **********

 

The customer is requesting that we make pads similar to pads on other

parts, but properly sized for the DL-35 part.

 

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2