You mean not flash? You are one of few complain about too much gold for the same price nowadays. With gold price so high, bonding wire getting thinner, or change to copper wire.
--------------------------
Sent using BlackBerry
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Fri Oct 03 05:05:55 2008
Subject: Re: [TN] Electrolytic (Flash) Nickel Gold Finish
If the flash gold is indeed thin, than there is no reliability difference. However, imAu is self-limiting, flash Au is not. The only true Au-embrittlement I have seen in recent history was with flash-Au plated too thick.
Werner
-----Ursprüngliche Mitteilung-----
Von: Lee parker <[log in to unmask]>
An: [log in to unmask]
Verschickt: Do., 2. Okt. 2008, 16:01
Thema: Re: [TN] Electrolytic (Flash) Nickel Gold Finish
Arnaud
I have not seen any definitive side by side data comparing the reliability
f ENIG and flash gold. Perhaps a vendor in Asia could make this comparison.
have worked with OEMs using both coatings, but from different suppliers.
lash gold was found to be a better choice (fewer quality issues).
Process control is operating the process in a manner consistent with the
uppliers specification. When I audit a shop I request a copy of the
hemical suppliers specification for each bath. In cases, I have found that
he PCB supplier did not have these instructions. In other cases the process
as not being operated according to the suppliers specification. In the case
f ENIG this can cause porous gold or even black pad. Unfortunately,
uditing incoming product is a must to maintained a high quality product.
he auditing frequency should be a function of the product's complexity and
he OEMs long term experience with the PCB supplier. Initially the frequency
hould be 100%. As confidence in the supplier increases, the frequency can
sually be reduced.
Best regards
ee
LP Consultants LLC
04 779 3389
---- Original Message -----
rom: "arnaud grivon" <[log in to unmask]>
o: "TechNet E-Mail Forum" <[log in to unmask]>; "Lee parker" <[log in to unmask]>
ent: Thursday, October 02, 2008 5:05 AM
ubject: Re: [TN] Electrolytic (Flash) Nickel Gold Finish
ee,
Could you elaborate on the kind of 'serious' problems we can have with
l wedge wire bonding + flash Au plating?
hat effects are you referring to and what shall be controlled in the Au
rocess?
have had one case where usual controls including pull tests were not
ufficient to detect a 'serious' problem due to the flash Au finish.
would echo Inge and say that ENIG is safer.
Arnaud Grivon
Lee parker a écrit :
Anand
Flash gold plating is widely available in Asia and is being used as a
alternative to ENIG. This has been in place since early 2000s. The
thickness
is about 2 micro inches. I have worked with several OEMs using this
coating
for aluminum wire bonding and the results have been positive. Of course,
if
the process is not properly controlled, you may have serious problems. I
always recommend continuing due diligence and incoming inspection with any
supplier.
Best regards
Lee
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Anand" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, October 01, 2008 5:02 PM
Subject: [TN] Electrolytic (Flash) Nickel Gold Finish
Hi All,
I want to use Alluminum WEDGE wire bonding for COB.
as the ENIG i
s suitable only for Gold Wire Bonding .....! which i don't
want.
I thought about Electrolytic (Flash) Nickel Gold Finish. as alluminum wire
bond
can be used.
but i don;t know the recommended thickness of nickel and Gold for
A) Electrolytic ?????? I didn't found any ipc std for this ?
B) Can any ONE please guide me for the thickness of this plating....!
C) again as there is no phosphurus used in electrlytic process how can we
prevent the corrosion for this plating ?
thanks and eagerly waiting for the answer on above three questions .....
Regards,
Anand
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask]
with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
dditional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
________________________________________________________________________
AOL eMail auf Ihrem Handy! Ab sofort können Sie auch unterwegs Ihre AOL email abrufen. Registrieren Sie sich jetzt kostenlos.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|