I am confused.
i have some chart which shows block of gold plating then HASL/HAL.
i am trying to understand if it is by mistake showing HASL after Gold
Plating ?
or some Fabricator actually using HASL/HAL Process after Gold plating
Process ? if yes why did they required to do that ?
Thanks
Regards,
Anand
On Tue, Oct 14, 2008 at 12:28 PM, Lee Whiteman
<[log in to unmask]>wrote:
> Roger,
>
> I never heard of HASL over gold. I am assuming that the gold is
> deposited (?) over the copper pads, then HASL is performed.
>
> What are the advantages of this finish over ENIG and straight HASL?
>
> Why would a board be finished like that? Just curious.
>
> Lee Whiteman, PMP
> Senior Member Engineering Staff
> L-3 Communications East
> Telephone: (856) 338-3508
> FAX: (856) 338-2906
> E-Mail: [log in to unmask]
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Roger Stoops
> Sent: Tuesday, October 14, 2008 2:22 PM
> To: [log in to unmask]
> Subject: Re: [TN] Process question-Pls reply urgently....!
>
> Gold and silver are deposited by chemical methods. Solder, both
> lead-free and lead/tin, are deposited by HASL. HASL solder can be
> applied after gold finish, as in the case of gold-plated edge fingers.
>
> HASL = Hot Air Solder Leveling
>
> Roger
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of anand paliwal
> Sent: Tuesday, October 14, 2008 2:19 PM
> To: [log in to unmask]
> Subject: Re: [TN] Process question-Pls reply urgently....!
>
> could that melting metal would be the gold, silver, ?
>
> thanks for the reply
>
> regards,
> Anand
> On Tue, Oct 14, 2008 at 12:08 PM, <[log in to unmask]> wrote:
>
> >
> > Anand
> > HASL is not applied over other finishes, to the best of my knowledge.
>
> > HASL is a process for putting a melting metal onto a copper substrate.
> >
> > Doug Pauls
> > Rockwell Collins
> >
> >
> > *anand paliwal <[log in to unmask]>* Sent by: TechNet
> > <[log in to unmask]>
> >
> > 10/14/2008 12:40 PM Please respond to
> > TechNet E-Mail Forum <[log in to unmask]>; Please respond to anand
> > paliwal <[log in to unmask]>
> >
> > To
> > [log in to unmask] cc
> > Subject
> > [TN] Process question-Pls reply urgently....!
> >
> >
> >
> >
> > Hi All,
> >
> > I have One question Does the HASL Applied after gold plating ?
> >
> > is HASL can be used for Different Plating finish ?
> >
> > Thanks
> > --
> > With Best Regards,
> > Anand
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> > unsubscribe, send a message to [log in to unmask] with following text in
>
> > the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> > or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> > per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> > http://listserv.ipc.org/archives Please visit IPC web site
> > http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional
> > information, or contact Keach Sasamori at [log in to unmask] or
> > 847-615-7100 ext.2815
> > -----------------------------------------------------
> >
> >
>
>
> --
> With Best Regards,
> Anand Paliwal
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
--
With Best Regards,
Anand Paliwal
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|