Chip is cdse?
--------------------------
Sent using BlackBerry
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Sat Oct 11 04:56:55 2008
Subject: Re: [TN] Need soldering advice ASAP!
Hi Inge.
What die size?
I sincerely doubt you have Cadmium, can you be looking at spectral lines and
mistaking for Cd?
If you do have Cd it must be contamination. I can't think anyone would apply
it as a surface preserver on die. IF present it could easily change wetting
ability of solder/solderability.
The voiding would easily be caused by surface contamination, on either die
solder or substrate.
IS your Au/Sn clean? have you contaminated it by "cleaning" it in house?
Does happen.
Has parts/substrate packaging changed, or are parts being re-packed before
use. eg put in poly bags or something. How about something off the wall like
machine maintainence - someone using illicit spray on conveyor that sort of
thing.
As a diagnostic try burnishing parts on a piece of un metallised circuit
tile. Al2O3 is good abrasive and substrates are very flat.
Then if necessary -(serially for each surface -solvent degrease, DI wash ,
IPA de -water and then bake dry.
I am curious why the wire bonding fails, you can have serious voids before
affecting that. Could there be something else unrelated coincidentally going
on?
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Thursday, October 09, 2008 5:00 PM
To: [log in to unmask]
Subject: [TN] Need soldering advice ASAP!
Hi all, especially the Indi-man,
We have soldered IRC's power MOSFET (100-250 W) dice for a decade without
problems. They use to be vacuum soldered to a solderable gold thickfilm
Al2O3 substrate with AuSn 50 micrometer preforms. Now there is a production
stop because of Al heavy wire wedge bonding problems. My analysis of this
case points at the presence of large voids in the solder joints or maybe
partly dewetting (FineFocus is good but the resolution is not sufficient to
make me sure), something the US mechanical waves don't like. The die
backside is plated with something that I don't recognize: Cadmium over
Silver over Nickel. What the heck is that? Anyone who can figure out if AuSn
is the best preforms for that plating?
Thanks
/Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|